Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.6 g/cm³ Show Supplier Material materials with Dichte of 7.6 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 7 - 10 % Show Supplier Material materials with Dehnung of 7 - 10 % |
Elastizitätsmodul | 23.0 °C | 110 GPa Show Supplier Material materials with Elastizitätsmodul of 110 GPa |
Härte, Brinell | 23.0 °C | 225 [-] Show Supplier Material materials with Härte, Brinell of 225 [-] |
Härte, Rockwell C | 23.0 °C | 20 [-] Show Supplier Material materials with Härte, Rockwell C of 20 [-] |
Härte, Vickers | 23.0 °C | 227 [-] Show Supplier Material materials with Härte, Vickers of 227 [-] |
Streckgrenze | 23.0 °C | 540 - 590 MPa Show Supplier Material materials with Streckgrenze of 540 - 590 MPa |
Zugfestigkeit | 23.0 °C | 780 - 830 MPa Show Supplier Material materials with Zugfestigkeit of 780 - 830 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.7E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.7E-5 1/K | for 20-200°C |
Wärmeleitfähigkeit | 23.0 °C | 35 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 35 W/(m·K) | for 20-200°C |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 3.00E+6 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 3.00E+6 S/m |
Magnetisch
Property | Temperature | Value |
---|---|---|
Relative magnetische Permeabilität | 23.0 °C | 1.2 [-] Show Supplier Material materials with Relative magnetische Permeabilität of 1.2 [-] |
Technological properties
Property | ||
---|---|---|
Application areas | Summary of typical applications: Rings (friction-guidance) for landing gears | |
Corrosion properties | Corrosion resistance rating: 3 out of 5 | |
General machinability | Machinability: 30 % |