Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.36 g/cm³ Show Supplier Material materials with Dichte of 8.36 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 8 - 18 % Show Supplier Material materials with Dehnung of 8 - 18 % |
Elastizitätsmodul | 23.0 °C | 107 GPa Show Supplier Material materials with Elastizitätsmodul of 107 GPa |
Härte, Brinell | 23.0 °C | 103 - 170 [-] Show Supplier Material materials with Härte, Brinell of 103 - 170 [-] |
Härte, Rockwell C | 23.0 °C | 0 - 7 [-] Show Supplier Material materials with Härte, Rockwell C of 0 - 7 [-] |
Härte, Vickers | 23.0 °C | 110 - 175 [-] Show Supplier Material materials with Härte, Vickers of 110 - 175 [-] |
Streckgrenze | 23.0 °C | 220 - 570 MPa Show Supplier Material materials with Streckgrenze of 220 - 570 MPa |
Zugfestigkeit | 23.0 °C | 410 - 600 MPa Show Supplier Material materials with Zugfestigkeit of 410 - 600 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.1E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.1E-5 1/K | for 20-200°C |
Wärmeleitfähigkeit | 23.0 °C | 117 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 117 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 1.50E+7 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 1.50E+7 S/m |
Specific Electrical conductivity | 26 % IACS Show Supplier Material materials with Specific Electrical conductivity of 26 % IACS |