Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.65 g/cm³ Show Supplier Material materials with Dichte of 8.65 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 2 - 40 % Show Supplier Material materials with Dehnung of 2 - 40 % |
Elastizitätsmodul | 23.0 °C | 120 GPa Show Supplier Material materials with Elastizitätsmodul of 120 GPa |
Härte, Brinell | 23.0 °C | 80 - 199 [-] Show Supplier Material materials with Härte, Brinell of 80 - 199 [-] |
Härte, Rockwell C | 23.0 °C | 0 - 15 [-] Show Supplier Material materials with Härte, Rockwell C of 0 - 15 [-] |
Härte, Vickers | 23.0 °C | 90 - 200 [-] Show Supplier Material materials with Härte, Vickers of 90 - 200 [-] |
Streckgrenze | 23.0 °C | 140 - 550 MPa Show Supplier Material materials with Streckgrenze of 140 - 550 MPa |
Zugfestigkeit | 23.0 °C | 400 - 650 MPa Show Supplier Material materials with Zugfestigkeit of 400 - 650 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.6E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.6E-5 1/K | for 20-200°C |
Wärmeleitfähigkeit | 23.0 °C | 35 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 35 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 5.00E+6 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 5.00E+6 S/m |
Specific Electrical conductivity | 8 % IACS Show Supplier Material materials with Specific Electrical conductivity of 8 % IACS |
Technological properties
Property | ||
---|---|---|
Application areas | ball point pen tips | |
General machinability | 85 % |