Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.4 g/cm³ Show Supplier Material materials with Dichte of 8.4 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 3 - 38 % Show Supplier Material materials with Dehnung of 3 - 38 % |
Elastizitätsmodul | 23.0 °C | 115 GPa Show Supplier Material materials with Elastizitätsmodul of 115 GPa |
Härte, Brinell | 23.0 °C | 104 - 216 [-] Show Supplier Material materials with Härte, Brinell of 104 - 216 [-] |
Härte, Rockwell C | 23.0 °C | 1 - 19 [-] Show Supplier Material materials with Härte, Rockwell C of 1 - 19 [-] |
Härte, Vickers | 23.0 °C | 111 - 175 [-] Show Supplier Material materials with Härte, Vickers of 111 - 175 [-] |
Streckgrenze | 23.0 °C | 241 - 700 MPa Show Supplier Material materials with Streckgrenze of 241 - 700 MPa |
Zugfestigkeit | 23.0 °C | 491 - 780 MPa Show Supplier Material materials with Zugfestigkeit of 491 - 780 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.9E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.9E-5 1/K | for 20-200°C |
Wärmeleitfähigkeit | 23.0 °C | 33 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 33 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 4.00E+6 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 4.00E+6 S/m |
Specific Electrical conductivity | 7 % IACS Show Supplier Material materials with Specific Electrical conductivity of 7 % IACS |
Technological properties
Property | ||
---|---|---|
Application areas | ball point pen tips cold formed and machined eyeglass components screws | |
General machinability | 90 % |