Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.3 g/cm³ Show Supplier Material materials with Dichte of 8.3 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 1 - 30 % Show Supplier Material materials with Dehnung of 1 - 30 % |
Elastizitätsmodul | 23.0 °C | 120 GPa Show Supplier Material materials with Elastizitätsmodul of 120 GPa |
Härte, Brinell | 23.0 °C | 80 - 103 [-] Show Supplier Material materials with Härte, Brinell of 80 - 103 [-] |
Härte, Vickers | 23.0 °C | 90 - 110 [-] Show Supplier Material materials with Härte, Vickers of 90 - 110 [-] |
Streckgrenze | 23.0 °C | 250 - 720 MPa Show Supplier Material materials with Streckgrenze of 250 - 720 MPa |
Zugfestigkeit | 23.0 °C | 450 - 850 MPa Show Supplier Material materials with Zugfestigkeit of 450 - 850 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.9E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.9E-5 1/K | for 20-200°C |
Wärmeleitfähigkeit | 23.0 °C | 30 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 30 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 3.00E+6 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 3.00E+6 S/m |
Specific Electrical conductivity | 5 % IACS Show Supplier Material materials with Specific Electrical conductivity of 5 % IACS |
Technological properties
Property | ||
---|---|---|
Application areas | writing instruments components for fiber optic connectors components for high safety locks spare parts for eyeglasses | |
General machinability | 90 % |