Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.5 g/cm³ Show Supplier Material materials with Dichte of 8.5 g/cm³ |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.8E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.8E-5 1/K | for 20-200°C |
Wärmeleitfähigkeit | 23.0 °C | 34 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 34 W/(m·K) |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Temperaturwiderstandskoeffizient | -20.0 °C | -4E-5 1/K Show Supplier Material materials with Temperaturwiderstandskoeffizient of -4E-5 1/K | between -20 and +150°C |
150.0 °C | 4E-5 1/K Show Supplier Material materials with Temperaturwiderstandskoeffizient of 4E-5 1/K | between -20 and +150°C | |
Themo EMF | 23.0 °C | -3E-6 V/K Show Supplier Material materials with Themo EMF of -3E-6 V/K | against copper |
spezifischer Widerstand | 23.0 °C | 2.9E-7 Ω·m Show Supplier Material materials with spezifischer Widerstand of 2.9E-7 Ω·m |
Technological properties
Property | ||
---|---|---|
Application areas | Precision resistors / Electrical shunts |