Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.76 g/cm³ Show Supplier Material materials with Dichte of 8.76 g/cm³ |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.8E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.8E-5 1/K | for 20-200°C |
Wärmeleitfähigkeit | 23.0 °C | 22 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 22 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 23.0 °C | 4.2E-7 Ω·m Show Supplier Material materials with spezifischer Widerstand of 4.2E-7 Ω·m |
Technological properties
Property | ||
---|---|---|
Application areas | Precision resistors / Electrical shunts in electricity meters / Electrical shunts in DC ammeters |