Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.76 g/cm³ Show Supplier Material materials with Dichte of 8.76 g/cm³ |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.8E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.8E-5 1/K | for 20-200°C |
Wärmeleitfähigkeit | 23.0 °C | 22 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 22 W/(m·K) |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Temperaturwiderstandskoeffizient | -20.0 °C | -1.5E-5 1/K Show Supplier Material materials with Temperaturwiderstandskoeffizient of -1.5E-5 1/K | between -20 and +150°C |
150.0 °C | 1.5E-5 1/K Show Supplier Material materials with Temperaturwiderstandskoeffizient of 1.5E-5 1/K | between -20 and +150°C | |
Themo EMF | 23.0 °C | -9.8E-7 V/K Show Supplier Material materials with Themo EMF of -9.8E-7 V/K | against copper |
spezifischer Widerstand | 23.0 °C | 4.3E-7 Ω·m Show Supplier Material materials with spezifischer Widerstand of 4.3E-7 Ω·m |
Technological properties
Property | ||
---|---|---|
Application areas | Precision resistors - Electrical shunts in electricity meter - Electrical shunts in DC ammeters |