Thermisch
Property | Value |
---|---|
Glasübergangstemperatur | -28.0 °C Show Supplier Material materials with Glasübergangstemperatur of -28.0 °C |
Rheological Properties
Property | Value |
---|---|
Mooney-Viskosität | 50 MU Show Supplier Material materials with Mooney-Viskosität of 50 MU |
Technological properties
Property | ||
---|---|---|
Application areas | Performance, High performance tire | |
Chemical composition | Styrene: 25% Vinyl: 50% Extended Oil: TDAE Oil: 37.5 phr | |
Other | It should be stored in warehouse to be protected from sunlight, heat and moisture. Shelf life : 24 months from date of production at room temperature not exceeding 30°C under above storage condition. (Retest critical parameters like MV and others after the expiry of shelf life) |