Rheological Properties
Property | Value |
---|---|
Mooney-Viskosität | 45 MU Show Supplier Material materials with Mooney-Viskosität of 45 MU |
Technological properties
Property | ||
---|---|---|
Application areas | Processability, Wear resistance, Cold resistance (Tire, Belt) | |
Other | It should be stored in warehouse to be protected from sunlight, heat and moisture. Shelf life : 24 months from date of production at room temperature not exceeding 30°C under above storage condition. (Retest critical parameters like MV and others after the expiry of shelf life) | |
Processing history | Catalyst: nickel |