Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 2.92 g/cm³ Show Supplier Material materials with Dichte of 2.92 g/cm³ |
Korngröße | 22 μm Show Supplier Material materials with Korngröße of 22 μm | |
Wasserabsorption | 23.0 °C | 0 % Show Supplier Material materials with Wasserabsorption of 0 % |
Mechanisch
Property | Temperature | Value |
---|---|---|
Biegefestigkeit | 23.0 °C | 207 MPa Show Supplier Material materials with Biegefestigkeit of 207 MPa |
Druckfestigkeit | 23.0 °C | 1.55 MPa Show Supplier Material materials with Druckfestigkeit of 1.55 MPa |
Elastizitätsmodul | 23.0 °C | 345 GPa Show Supplier Material materials with Elastizitätsmodul of 345 GPa |
Hardness, Rockwell Superficial 45-N | 23.0 °C | 60 [-] Show Supplier Material materials with Hardness, Rockwell Superficial 45-N of 60 [-] |
Plane-Strain Fracture Toughnes | 23.0 °C | 3.5 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 3.5 MPa·√m |
Poissonzahl | 23.0 °C | 0.26 [-] Show Supplier Material materials with Poissonzahl of 0.26 [-] |
Zugfestigkeit | 23.0 °C | 152 MPa Show Supplier Material materials with Zugfestigkeit of 152 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 9E-6 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 9E-6 1/K |
Spezifische Wärmekapazität | 23.0 °C | 1046 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 1046 J/(kg·K) |
Wärmeleitfähigkeit | 23.0 °C | 325 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 325 W/(m·K) |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 10GHz | 23.0 °C | 6.76 [-] Show Supplier Material materials with Dielectric constant, 10GHz of 6.76 [-] | |
Dielektrizitätskonstante, 1 MHz | 23.0 °C | 6.76 [-] Show Supplier Material materials with Dielektrizitätskonstante, 1 MHz of 6.76 [-] | |
Dissipation factor, 1MHz | 23.0 °C | 4E-4 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 4E-4 [-] | |
Durchschlagfestigkeit | 23.0 °C | 0.23 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 0.23 kV/mm | AC, 6.35mm |
spezifischer Widerstand | 23.0 °C | 1.00E+13 Ω·m Show Supplier Material materials with spezifischer Widerstand of 1.00E+13 Ω·m | Minimum |
Technological properties
Property | ||
---|---|---|
Application areas | Diode lasers, Medical scanning equipment, Semiconductor substrates, Automotive ignition systems, Thick film circuits, Components for missile guidance, Radio frequency transmitters | |
Color | Light Grey |