Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 3.95 g/cm³ Show Supplier Material materials with Dichte of 3.95 g/cm³ |
Korngröße | 1 μm Show Supplier Material materials with Korngröße of 1 μm | |
Wasserabsorption | 23.0 °C | 0 % Show Supplier Material materials with Wasserabsorption of 0 % |
Mechanisch
Property | Temperature | Value |
---|---|---|
Biegefestigkeit | 23.0 °C | 379 MPa Show Supplier Material materials with Biegefestigkeit of 379 MPa |
Druckfestigkeit | 23.0 °C | 2.41 MPa Show Supplier Material materials with Druckfestigkeit of 2.41 MPa |
Elastizitätsmodul | 23.0 °C | 375 GPa Show Supplier Material materials with Elastizitätsmodul of 375 GPa |
Hardness, Rockwell Superficial 45-N | 23.0 °C | 85 [-] Show Supplier Material materials with Hardness, Rockwell Superficial 45-N of 85 [-] |
Plane-Strain Fracture Toughnes | 23.0 °C | 4 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 4 MPa·√m |
Poissonzahl | 23.0 °C | 0.22 [-] Show Supplier Material materials with Poissonzahl of 0.22 [-] |
Zugfestigkeit | 23.0 °C | 276 MPa Show Supplier Material materials with Zugfestigkeit of 276 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 8E-6 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 8E-6 1/K | RT to 1000°C |
Spezifische Wärmekapazität | 23.0 °C | 837.36 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 837.36 J/(kg·K) | |
Wärmeleitfähigkeit | 23.0 °C | 35 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 35 W/(m·K) |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 10GHz | 23.0 °C | 9.6 [-] Show Supplier Material materials with Dielectric constant, 10GHz of 9.6 [-] | |
Dielektrizitätskonstante, 1 MHz | 23.0 °C | 9.7 [-] Show Supplier Material materials with Dielektrizitätskonstante, 1 MHz of 9.7 [-] | |
Dissipation factor, 1MHz | 23.0 °C | 1E-4 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 1E-4 [-] | |
Durchschlagfestigkeit | 23.0 °C | 0.22 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 0.22 kV/mm | AC, 6.35mm |
spezifischer Widerstand | 23.0 °C | 1.00E+13 Ω·m Show Supplier Material materials with spezifischer Widerstand of 1.00E+13 Ω·m | Minimum |
Technological properties
Property | ||
---|---|---|
Application areas | photonics/ lasers, defense, energy, telecommunications and semiconductor manufacturing | |
Color | White |