Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 9 g/cm³ Show Supplier Material materials with Dichte of 9 g/cm³ |
Abmessung
Property | Value | Comment |
---|---|---|
Durchmesser | 6.35 - 10 mm Show Supplier Material materials with Durchmesser of 6.35 - 10 mm | also for less than 6.35mm |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 5 - 7 % Show Supplier Material materials with Dehnung of 5 - 7 % | in 4D |
Elastizitätsmodul | 23.0 °C | 144 GPa Show Supplier Material materials with Elastizitätsmodul of 144 GPa | |
Härte, Rockwell C | 23.0 °C | 32 [-] Show Supplier Material materials with Härte, Rockwell C of 32 [-] | |
Poissonzahl | 23.0 °C | 0.33 [-] Show Supplier Material materials with Poissonzahl of 0.33 [-] | |
Streckgrenze Rp 0,2 | 23.0 °C | 1035 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 1035 MPa | |
Zugfestigkeit | 23.0 °C | 1105 MPa Show Supplier Material materials with Zugfestigkeit of 1105 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.64E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.64E-5 1/K |
Wärmeleitfähigkeit | 23.0 °C | 38 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 38 W/(m·K) |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 4.00E+6 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 4.00E+6 S/m | max. |
Specific Electrical conductivity | 7 % IACS Show Supplier Material materials with Specific Electrical conductivity of 7 % IACS | max. |
Magnetisch
Property | Temperature | Value |
---|---|---|
Relative magnetische Permeabilität | 23.0 °C | 1 [-] Show Supplier Material materials with Relative magnetische Permeabilität of 1 [-] |
Technological properties
Property | ||
---|---|---|
Application areas | ToughMet 3 TS alloy tempers are commonly used in the oil and gas industry, oil & gas production via our sucker rod couplings and in commercial aircraft. |