Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 9 g/cm³ Show Supplier Material materials with Dichte of 9 g/cm³ |
Abmessung
Property | Value |
---|---|
Außendurchmesser | 28.6 - 254 mm Show Supplier Material materials with Außendurchmesser of 28.6 - 254 mm |
Innendurchmesser | 12.7 - 76.2 mm Show Supplier Material materials with Innendurchmesser of 12.7 - 76.2 mm |
Wall thickness | 6.35 - 15.9 mm Show Supplier Material materials with Wall thickness of 6.35 - 15.9 mm |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dauerfestigkeit | 23.0 °C | 413 MPa Show Supplier Material materials with Dauerfestigkeit of 413 MPa | 10⁶ cycles R=-1 |
Dehnung | 23.0 °C | 6 % Show Supplier Material materials with Dehnung of 6 % | |
Elastizitätsmodul | 23.0 °C | 144 GPa Show Supplier Material materials with Elastizitätsmodul of 144 GPa | |
Härte, Rockwell C | 23.0 °C | 27 [-] Show Supplier Material materials with Härte, Rockwell C of 27 [-] | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Supplier Material materials with Poissonzahl of 0.3 [-] | |
Streckgrenze Rp 0,2 | 23.0 °C | 621 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 621 MPa | |
Zugfestigkeit | 23.0 °C | 724 MPa Show Supplier Material materials with Zugfestigkeit of 724 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.6E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.6E-5 1/K |
Wärmeleitfähigkeit | 23.0 °C | 38 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 38 W/(m·K) |
Elektrisch
Property | Value |
---|---|
Specific Electrical conductivity | 9 % IACS Show Supplier Material materials with Specific Electrical conductivity of 9 % IACS |
Magnetisch
Property | Temperature | Value |
---|---|---|
Relative magnetische Permeabilität | 23.0 °C | 1 [-] Show Supplier Material materials with Relative magnetische Permeabilität of 1 [-] |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | ToughMet 3 CX alloy is used for wear plates, bushings, sleeve bearings, linear bearings and thrust bearings in industrial, off-road, mining and heavy equipment. It is also used for oil and gas drilling hardware. |