Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.36 g/cm³ Show Supplier Material materials with Dichte of 8.36 g/cm³ |
Abmessung
Property | Value |
---|---|
Breite | 1.27 - 406.5 mm Show Supplier Material materials with Breite of 1.27 - 406.5 mm |
Dicke | 0.05 - 1.61 mm Show Supplier Material materials with Dicke of 0.05 - 1.61 mm |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefähigkeit 90°, in longitudinaler Richtung | 23.0 °C | 0 [-] Show Supplier Material materials with Biegefähigkeit 90°, in longitudinaler Richtung of 0 [-] | for strip with 0.25mm and thinner. |
Biegefähigkeit 90°, in transversaler Richtung | 23.0 °C | 0 [-] Show Supplier Material materials with Biegefähigkeit 90°, in transversaler Richtung of 0 [-] | for strip with 0.25mm and thinner. |
Dehnung | 23.0 °C | 16 - 30 % Show Supplier Material materials with Dehnung of 16 - 30 % | min., for strip thicker than 0.10 mm |
Elastizitätsmodul | 23.0 °C | 131 GPa Show Supplier Material materials with Elastizitätsmodul of 131 GPa | |
Härte, Vickers | 23.0 °C | 210 - 251 [-] Show Supplier Material materials with Härte, Vickers of 210 - 251 [-] | |
Streckgrenze Rp 0,2 | 23.0 °C | 480 - 660 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 480 - 660 MPa | |
Zugfestigkeit | 23.0 °C | 690 - 760 MPa Show Supplier Material materials with Zugfestigkeit of 690 - 760 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.75E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.75E-5 1/K |
Schmelzpunkt | 870 °C Show Supplier Material materials with Schmelzpunkt of 870 °C | |
Wärmeleitfähigkeit | 23.0 °C | 105 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 105 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Specific Electrical conductivity | 17 - 28 % IACS Show Supplier Material materials with Specific Electrical conductivity of 17 - 28 % IACS | |
spezifischer Widerstand | 23.0 °C | 6.2E-8 - 1.01E-7 Ω·m Show Supplier Material materials with spezifischer Widerstand of 6.2E-8 - 1.01E-7 Ω·m |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Beryllium | 1.8 - 2.2 % Show Supplier Material materials with Beryllium of 1.8 - 2.2 % | ||
Eisen | 0.6 % Show Supplier Material materials with Eisen of 0.6 % | max., Nickel + Cobalt + Iron | |
Kobalt | 0.2 % Show Supplier Material materials with Kobalt of 0.2 % | min. Nickel + Cobalt | |
Kupfer | Balance | ||
Nickel | 0.2 % Show Supplier Material materials with Nickel of 0.2 % | min. Nickel + Cobalt |
Technological properties
Property | ||
---|---|---|
Application areas | Typical applications include high reliability spring contacts for switches and relays, battery contacts, and automotive terminals. |