Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.88 g/cm³ Show Supplier Material materials with Dichte of 8.88 g/cm³ |
Abmessung
Property | Value |
---|---|
Durchmesser | 0.76 - 15.8 mm Show Supplier Material materials with Durchmesser of 0.76 - 15.8 mm |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 4 - 30 % Show Supplier Material materials with Dehnung of 4 - 30 % |
Streckgrenze Rp 0,2 | 23.0 °C | 380 - 660 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 380 - 660 MPa |
Zugfestigkeit | 23.0 °C | 480 - 720 MPa Show Supplier Material materials with Zugfestigkeit of 480 - 720 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.77E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.77E-5 1/K |
Wärmeleitfähigkeit | 23.0 °C | 210 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 210 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 2.90E+7 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 2.90E+7 S/m |
Specific Electrical conductivity | 50 % IACS Show Supplier Material materials with Specific Electrical conductivity of 50 % IACS |
Chemical properties
Property | Value |
---|---|
Blei | 0.8 - 1.2 % Show Supplier Material materials with Blei of 0.8 - 1.2 % |
Kupfer | Balance |
Nickel | 0.8 - 1.2 % Show Supplier Material materials with Nickel of 0.8 - 1.2 % |
Phosphor | 0.15 - 0.35 % Show Supplier Material materials with Phosphor of 0.15 - 0.35 % |
Technological properties
Property | ||
---|---|---|
Application areas | Brush 1916 is a strong material to machine or form into electrical contacts, connector pins and sockets. | |
General machinability | The addition of lead in the Brush 1915 & Brush 1916 alloy composition allows for chip control in turning and drilling operations, making the alloy ideal for automatic machining. Brush 1915 & Brush 1916 machines readily at feeds and speeds used for other leaded copper alloys. High speed steel and carbide tools are recommended for all machining operations. |