Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.36 g/cm³ Show Supplier Material materials with Dichte of 8.36 g/cm³ |
Abmessung
Property | Value | Comment |
---|---|---|
Durchmesser | 0.76 - 76 mm Show Supplier Material materials with Durchmesser of 0.76 - 76 mm | |
Länge | 91000 mm Show Supplier Material materials with Länge of 91000 mm | max. |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 8 - 30 % Show Supplier Material materials with Dehnung of 8 - 30 % |
Elastizitätsmodul | 23.0 °C | 131 GPa Show Supplier Material materials with Elastizitätsmodul of 131 GPa |
Streckgrenze Rp 0,2 | 23.0 °C | 520 - 720 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 520 - 720 MPa |
Zugfestigkeit | 23.0 °C | 590 - 900 MPa Show Supplier Material materials with Zugfestigkeit of 590 - 900 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.75E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.75E-5 1/K |
Schmelzpunkt | 870 °C Show Supplier Material materials with Schmelzpunkt of 870 °C | |
Wärmeleitfähigkeit | 23.0 °C | 105 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 105 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Specific Electrical conductivity | 25 - 30 % IACS Show Supplier Material materials with Specific Electrical conductivity of 25 - 30 % IACS | |
spezifischer Widerstand | 23.0 °C | 5.8E-6 - 6.9E-6 Ω·m Show Supplier Material materials with spezifischer Widerstand of 5.8E-6 - 6.9E-6 Ω·m |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Beryllium | 1.8 - 2 % Show Supplier Material materials with Beryllium of 1.8 - 2 % | ||
Eisen | 0.6 % Show Supplier Material materials with Eisen of 0.6 % | max., Nickel + Cobalt + Iron | |
Kobalt | 0.2 % Show Supplier Material materials with Kobalt of 0.2 % | min. Nickel + Cobalt | |
Kupfer | Balance | ||
Nickel | 0.2 % Show Supplier Material materials with Nickel of 0.2 % | min. Nickel + Cobalt |
Technological properties
Property | ||
---|---|---|
Application areas | Typical applications include downhole drilling flex shafts, bushings and bearings, circular and coaxial connectors, test probes and compression contacts. |