Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.36 g/cm³ Show Supplier Material materials with Dichte of 8.36 g/cm³ |
Abmessung
Property | Value |
---|---|
Durchmesser | 1.27 - 2 mm Show Supplier Material materials with Durchmesser of 1.27 - 2 mm |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 2 - 8 % Show Supplier Material materials with Dehnung of 2 - 8 % |
Elastizitätsmodul | 23.0 °C | 131 GPa Show Supplier Material materials with Elastizitätsmodul of 131 GPa |
Streckgrenze Rp 0,2 | 23.0 °C | 790 - 1040 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 790 - 1040 MPa |
Zugfestigkeit | 23.0 °C | 890 - 1070 MPa Show Supplier Material materials with Zugfestigkeit of 890 - 1070 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.75E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.75E-5 1/K |
Schmelzpunkt | 870 °C Show Supplier Material materials with Schmelzpunkt of 870 °C | |
Wärmeleitfähigkeit | 23.0 °C | 105 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 105 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Specific Electrical conductivity | 22 - 28 % IACS Show Supplier Material materials with Specific Electrical conductivity of 22 - 28 % IACS | |
spezifischer Widerstand | 23.0 °C | 6.2E-6 - 7.8E-6 Ω·m Show Supplier Material materials with spezifischer Widerstand of 6.2E-6 - 7.8E-6 Ω·m |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Beryllium | 1.8 - 2 % Show Supplier Material materials with Beryllium of 1.8 - 2 % | ||
Eisen | 0.6 % Show Supplier Material materials with Eisen of 0.6 % | max., Nickel + Cobalt + Iron | |
Kobalt | 0.2 % Show Supplier Material materials with Kobalt of 0.2 % | min. Nickel + Cobalt | |
Kupfer | Balance | ||
Nickel | 0.2 % Show Supplier Material materials with Nickel of 0.2 % | min. Nickel + Cobalt |
Technological properties
Property | ||
---|---|---|
Application areas | Typical applications include precision coil springs and pins for burn-in and test socket contacts and probe pins, computer processor socket contacts, cold headed fasteners, modular jack contacts, woven mesh electromagnetic shielding gaskets and resilient eyeglass frames. |