Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.5 g/cm³ Show Supplier Material materials with Dichte of 7.5 g/cm³ |
Abmessung
Property | Value | Comment | |
---|---|---|---|
Außendurchmesser | 406 mm Show Supplier Material materials with Außendurchmesser of 406 mm | max. | |
Länge | contact the supplier | ||
Wall thickness | Nominally 10-20% of OD |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 2 % Show Supplier Material materials with Dehnung of 2 % |
Elastizitätsmodul | 23.0 °C | 110 GPa Show Supplier Material materials with Elastizitätsmodul of 110 GPa |
Streckgrenze Rp 0,2 | 23.0 °C | 621 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 621 MPa |
Zugfestigkeit | 23.0 °C | 862 MPa Show Supplier Material materials with Zugfestigkeit of 862 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.6E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.6E-5 1/K |
Schmelzpunkt | 1040 °C Show Supplier Material materials with Schmelzpunkt of 1040 °C | |
Wärmeleitfähigkeit | 23.0 °C | 42 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 42 W/(m·K) |
Elektrisch
Magnetisch
Property | Temperature | Value |
---|---|---|
Relative magnetische Permeabilität | 23.0 °C | 1.1 - 1.2 [-] Show Supplier Material materials with Relative magnetische Permeabilität of 1.1 - 1.2 [-] |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 10.5 - 11.5 % Show Supplier Material materials with Aluminium of 10.5 - 11.5 % | |
Eisen | 4 - 5.5 % Show Supplier Material materials with Eisen of 4 - 5.5 % | |
Kupfer | 74.5 % Show Supplier Material materials with Kupfer of 74.5 % | |
Mangan | 1.5 % Show Supplier Material materials with Mangan of 1.5 % | max. |
Nickel | 4.2 - 6 % Show Supplier Material materials with Nickel of 4.2 - 6 % | |
Zink | 0.3 % Show Supplier Material materials with Zink of 0.3 % | max. |
Zinn | 0.25 % Show Supplier Material materials with Zinn of 0.25 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace applications, including, but not limited to: bushings, spherical and rod end bearings, rub pads, and wear strips. They are also commonly used for applications in the oil & gas and other durable goods markets. |