Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.85 g/cm³ Show Supplier Material materials with Dichte of 1.85 g/cm³ | Theoretical density for BeO: 0.9% |
Korngröße | 20 μm Show Supplier Material materials with Korngröße of 20 μm | max., ASTM E-112 |
Mechanisch
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.05 % Show Supplier Material materials with Aluminium of 0.05 % | max. |
Andere | 0.04 % Show Supplier Material materials with Andere of 0.04 % | max., other metallic impurities each |
Beryllium | 99.2 % Show Supplier Material materials with Beryllium of 99.2 % | min., BeO: 0.9% max |
Blei | 5E-3 % Show Supplier Material materials with Blei of 5E-3 % | max. |
Chrom | 0.01 % Show Supplier Material materials with Chrom of 0.01 % | max. |
Eisen | 0.08 % Show Supplier Material materials with Eisen of 0.08 % | max. |
Kalzium | 5E-3 % Show Supplier Material materials with Kalzium of 5E-3 % | max. |
Kobalt | 5E-3 % Show Supplier Material materials with Kobalt of 5E-3 % | max. |
Kohlenstoff | 0.09 % Show Supplier Material materials with Kohlenstoff of 0.09 % | max. |
Kupfer | 0.03 % Show Supplier Material materials with Kupfer of 0.03 % | max. |
Magnesium | 0.01 % Show Supplier Material materials with Magnesium of 0.01 % | max. |
Mangan | 5E-3 % Show Supplier Material materials with Mangan of 5E-3 % | max. |
Molybdän | 5E-3 % Show Supplier Material materials with Molybdän of 5E-3 % | max. |
Nickel | 0.03 % Show Supplier Material materials with Nickel of 0.03 % | max. |
Silber | 5E-3 % Show Supplier Material materials with Silber of 5E-3 % | max. |
Silizium | 0.05 % Show Supplier Material materials with Silizium of 0.05 % | max. |
Titan | 0.03 % Show Supplier Material materials with Titan of 0.03 % | max. |
Uran | 0.02 % Show Supplier Material materials with Uran of 0.02 % | max. |
Zink | 5E-3 % Show Supplier Material materials with Zink of 5E-3 % | max. |
Zirkonium | 0.03 % Show Supplier Material materials with Zirkonium of 0.03 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | It is used for nuclear test reactors and fusion walls due to their neutron reflectivity, neutron kinetic energy absorption, neutron kinetic energy absorption and high purity. |