Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.86 g/cm³ Show Supplier Material materials with Dichte of 1.86 g/cm³ | Theoretical density for BeO: 2.2% |
Korngröße | 15 μm Show Supplier Material materials with Korngröße of 15 μm | max., ASTM E-112 |
Mechanisch
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.1 % Show Supplier Material materials with Aluminium of 0.1 % | max. |
Andere | 0.04 % Show Supplier Material materials with Andere of 0.04 % | max., other metallic impurities each |
Beryllium | 98 % Show Supplier Material materials with Beryllium of 98 % | min., BeO: 2.2% max |
Eisen | 0.15 % Show Supplier Material materials with Eisen of 0.15 % | max. |
Kohlenstoff | 0.15 % Show Supplier Material materials with Kohlenstoff of 0.15 % | max. |
Magnesium | 0.08 % Show Supplier Material materials with Magnesium of 0.08 % | max. |
Silizium | 0.08 % Show Supplier Material materials with Silizium of 0.08 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | It is hot isostatically pressed beryllium grades used in space applications and for low-density, bare polished optical applications or when reduced weight is required. |