Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.89 g/cm³ Show Supplier Material materials with Dichte of 8.89 g/cm³ |
Abmessung
Property | Value | Comment |
---|---|---|
Dicke | 0.2 - 0.8 mm Show Supplier Material materials with Dicke of 0.2 - 0.8 mm | gauge |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefähigkeit 90°, in longitudinaler Richtung | 23.0 °C | 0.2 [-] Show Supplier Material materials with Biegefähigkeit 90°, in longitudinaler Richtung of 0.2 [-] | |
Biegefähigkeit 90°, in transversaler Richtung | 23.0 °C | 0.2 [-] Show Supplier Material materials with Biegefähigkeit 90°, in transversaler Richtung of 0.2 [-] | |
Dehnung | 23.0 °C | 5 - 9 % Show Supplier Material materials with Dehnung of 5 - 9 % | for strip thicker than 0.10 mm |
Elastizitätsmodul | 23.0 °C | 137 - 152 GPa Show Supplier Material materials with Elastizitätsmodul of 137 - 152 GPa | |
Härte, Vickers | 23.0 °C | 130 - 170 [-] Show Supplier Material materials with Härte, Vickers of 130 - 170 [-] | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Supplier Material materials with Poissonzahl of 0.3 [-] | |
Streckgrenze Rp 0,2 | 23.0 °C | 500 - 536 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 500 - 536 MPa | |
Zugfestigkeit | 23.0 °C | 538 - 558 MPa Show Supplier Material materials with Zugfestigkeit of 538 - 558 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.8E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.8E-5 1/K |
Wärmeleitfähigkeit | 23.0 °C | 341 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 341 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 4.70E+7 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 4.70E+7 S/m |
Specific Electrical conductivity | 78 - 81 % IACS Show Supplier Material materials with Specific Electrical conductivity of 78 - 81 % IACS |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 0.5 - 3 % Show Supplier Material materials with Chrom of 0.5 - 3 % | Ni+Si+Cr |
Kupfer | 99.5 % Show Supplier Material materials with Kupfer of 99.5 % | min. |
Nickel | 0.5 - 3 % Show Supplier Material materials with Nickel of 0.5 - 3 % | Ni+Si+Cr |
Silizium | 0.5 - 3 % Show Supplier Material materials with Silizium of 0.5 - 3 % | Ni+Si+Cr |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive Wire Harness Terminals and High Voltage Connectors, EV Charging Contacts, Appliance Power Contacts, Computer Power Contacts, Backplane, Midplane and Card Edge Connectors, Photovoltaic System Connectors, Heat Spreading for Consumer Electronics |