Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.83 g/cm³ Show Supplier Material materials with Dichte of 8.83 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 15 % Show Supplier Material materials with Dehnung of 15 % |
Elastizitätsmodul | 23.0 °C | 138 GPa Show Supplier Material materials with Elastizitätsmodul of 138 GPa |
Härte, Rockwell B | 23.0 °C | 97 [-] Show Supplier Material materials with Härte, Rockwell B of 97 [-] |
Härte, Rockwell C | 23.0 °C | 20 [-] Show Supplier Material materials with Härte, Rockwell C of 20 [-] |
Kerbschlagenergie | 23.0 °C | 55 J Show Supplier Material materials with Kerbschlagenergie of 55 J |
Streckgrenze Rp 0,2 | 23.0 °C | 620 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 620 MPa |
Zugfestigkeit | 23.0 °C | 725 MPa Show Supplier Material materials with Zugfestigkeit of 725 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.8E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.8E-5 1/K |
Schmelzpunkt | 1040 °C Show Supplier Material materials with Schmelzpunkt of 1040 °C | |
Spezifische Wärmekapazität | 100.0 °C | 410 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 410 J/(kg·K) |
Wärmeleitfähigkeit | 100.0 °C | 250 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 250 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Beryllium | 0.2 - 0.6 % Show Supplier Material materials with Beryllium of 0.2 - 0.6 % |
Kupfer | Balance |
Nickel | 1.4 - 2.2 % Show Supplier Material materials with Nickel of 1.4 - 2.2 % |
Technological properties
Property | ||
---|---|---|
Application areas | PROtherm alloy is used as blow mold cavities, injection mold cores and cavities and hot runners. |