Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.36 g/cm³ Show Supplier Material materials with Dichte of 8.36 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dauerfestigkeit | 23.0 °C | 310 MPa Show Supplier Material materials with Dauerfestigkeit of 310 MPa | 10⁷ cycles, R=-1 |
Dehnung | 23.0 °C | 5 % Show Supplier Material materials with Dehnung of 5 % | |
Elastizitätsmodul | 23.0 °C | 131 GPa Show Supplier Material materials with Elastizitätsmodul of 131 GPa | |
Härte, Rockwell C | 23.0 °C | 40 [-] Show Supplier Material materials with Härte, Rockwell C of 40 [-] | |
Kerbschlagenergie | 23.0 °C | 7 J Show Supplier Material materials with Kerbschlagenergie of 7 J | |
Streckgrenze Rp 0,2 | 23.0 °C | 1000 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 1000 MPa | |
Zugfestigkeit | 23.0 °C | 1170 MPa Show Supplier Material materials with Zugfestigkeit of 1170 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.75E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.75E-5 1/K |
Schmelzpunkt | 870 °C Show Supplier Material materials with Schmelzpunkt of 870 °C | |
Spezifische Wärmekapazität | 100.0 °C | 420 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 420 J/(kg·K) |
Wärmeleitfähigkeit | 100.0 °C | 130 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 130 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Beryllium | 1.6 - 2 % Show Supplier Material materials with Beryllium of 1.6 - 2 % |
Kobalt | 0.2 - 0.3 % Show Supplier Material materials with Kobalt of 0.2 - 0.3 % |
Kupfer | Balance |
Technological properties
Property | ||
---|---|---|
Application areas | MoldMAX HH Alloy is used for injection mold cores and cavities and blow mold pinch-offs. |