Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.69 g/cm³ Show Supplier Material materials with Dichte of 8.69 g/cm³ |
Abmessung
Property | Value |
---|---|
Durchmesser | 12.5 - 63.5 mm Show Supplier Material materials with Durchmesser of 12.5 - 63.5 mm |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dauerfestigkeit | 23.0 °C | 275 MPa Show Supplier Material materials with Dauerfestigkeit of 275 MPa | 10⁷ cycles, R=-1 |
Dehnung | 23.0 °C | 5 - 7 % Show Supplier Material materials with Dehnung of 5 - 7 % | |
Elastizitätsmodul | 23.0 °C | 130 GPa Show Supplier Material materials with Elastizitätsmodul of 130 GPa | |
Härte, HBW | 23.0 °C | 250 - 265 [-] Show Supplier Material materials with Härte, HBW of 250 - 265 [-] | |
Härte, Rockwell C | 23.0 °C | 25 - 27 [-] Show Supplier Material materials with Härte, Rockwell C of 25 - 27 [-] | HRC values converted per ASTM-E-140, Table 1. |
Kerbschlagenergie | 23.0 °C | 7 J Show Supplier Material materials with Kerbschlagenergie of 7 J | |
Streckgrenze Rp 0,2 | 23.0 °C | 690 - 790 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 690 - 790 MPa | |
Zugfestigkeit | 23.0 °C | 790 - 860 MPa Show Supplier Material materials with Zugfestigkeit of 790 - 860 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.75E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.75E-5 1/K |
Schmelzpunkt | 980 °C Show Supplier Material materials with Schmelzpunkt of 980 °C | |
Spezifische Wärmekapazität | 100.0 °C | 410 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 410 J/(kg·K) |
Wärmeleitfähigkeit | 100.0 °C | 160 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 160 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Chrom | 0.6 - 1.2 % Show Supplier Material materials with Chrom of 0.6 - 1.2 % |
Kupfer | Balance |
Nickel | 6.4 - 7.6 % Show Supplier Material materials with Nickel of 6.4 - 7.6 % |
Silizium | 1.5 - 2.5 % Show Supplier Material materials with Silizium of 1.5 - 2.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Applications include injection mold and blow mold cores and cavities. |