Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.83 g/cm³ Show Supplier Material materials with Dichte of 8.83 g/cm³ |
Abmessung
Property | Value |
---|---|
Breite | 305 - 559 mm Show Supplier Material materials with Breite of 305 - 559 mm |
Dicke | 44.5 - 127 mm Show Supplier Material materials with Dicke of 44.5 - 127 mm |
Länge | 610 - 3200 mm Show Supplier Material materials with Länge of 610 - 3200 mm |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 8 - 20 % Show Supplier Material materials with Dehnung of 8 - 20 % |
Elastizitätsmodul | 23.0 °C | 138 GPa Show Supplier Material materials with Elastizitätsmodul of 138 GPa |
Streckgrenze Rp 0,2 | 23.0 °C | 550 - 690 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 550 - 690 MPa |
Zugfestigkeit | 23.0 °C | 690 - 900 MPa Show Supplier Material materials with Zugfestigkeit of 690 - 900 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.76E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.76E-5 1/K |
Schmelzpunkt | 1040 °C Show Supplier Material materials with Schmelzpunkt of 1040 °C | |
Wärmeleitfähigkeit | 23.0 °C | 240 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 240 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Specific Electrical conductivity | 45 - 60 % IACS Show Supplier Material materials with Specific Electrical conductivity of 45 - 60 % IACS | |
spezifischer Widerstand | 23.0 °C | 2.9E-6 - 3.8E-6 Ω·m Show Supplier Material materials with spezifischer Widerstand of 2.9E-6 - 3.8E-6 Ω·m |
Chemical properties
Property | Value |
---|---|
Beryllium | 0.2 - 0.6 % Show Supplier Material materials with Beryllium of 0.2 - 0.6 % |
Kupfer | Balance |
Nickel | 1.4 - 2.2 % Show Supplier Material materials with Nickel of 1.4 - 2.2 % |
Technological properties
Property | ||
---|---|---|
Application areas | Typical applications include resistance welding components, and inserts for metal die casting, injection molding and blow molding. |