Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.8 g/cm³ Show Supplier Material materials with Dichte of 8.8 g/cm³ |
Abmessung
Property | Value |
---|---|
Breite | 1.27 - 406.5 mm Show Supplier Material materials with Breite of 1.27 - 406.5 mm |
Dicke | 0.05 - 2 mm Show Supplier Material materials with Dicke of 0.05 - 2 mm |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefähigkeit 90°, in longitudinaler Richtung | 23.0 °C | 0.5 [-] Show Supplier Material materials with Biegefähigkeit 90°, in longitudinaler Richtung of 0.5 [-] | for strip with 0.25mm and thinner. |
Biegefähigkeit 90°, in transversaler Richtung | 23.0 °C | 0.5 [-] Show Supplier Material materials with Biegefähigkeit 90°, in transversaler Richtung of 0.5 [-] | for strip with 0.25mm and thinner. |
Dauerfestigkeit | 23.0 °C | 515 - 585 MPa Show Supplier Material materials with Dauerfestigkeit of 515 - 585 MPa | 10⁸ cycles R=0 (Unidirectional) |
Dehnung | 23.0 °C | 10 - 20 % Show Supplier Material materials with Dehnung of 10 - 20 % | |
Elastizitätsmodul | 23.0 °C | 138 GPa Show Supplier Material materials with Elastizitätsmodul of 138 GPa | |
Härte, Vickers | 23.0 °C | 180 - 230 [-] Show Supplier Material materials with Härte, Vickers of 180 - 230 [-] | |
Streckgrenze Rp 0,2 | 23.0 °C | 550 - 690 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 550 - 690 MPa | |
Zugfestigkeit | 23.0 °C | 665 - 790 MPa Show Supplier Material materials with Zugfestigkeit of 665 - 790 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.76E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.76E-5 1/K |
Schmelzpunkt | 1020 °C Show Supplier Material materials with Schmelzpunkt of 1020 °C | |
Wärmeleitfähigkeit | 23.0 °C | 230 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 230 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Specific Electrical conductivity | 45 - 60 % IACS Show Supplier Material materials with Specific Electrical conductivity of 45 - 60 % IACS | |
spezifischer Widerstand | 23.0 °C | 2.9E-6 - 3.8E-6 Ω·m Show Supplier Material materials with spezifischer Widerstand of 2.9E-6 - 3.8E-6 Ω·m |
Chemical properties
Property | Value |
---|---|
Beryllium | 0.15 - 0.5 % Show Supplier Material materials with Beryllium of 0.15 - 0.5 % |
Kobalt | 0.35 - 0.6 % Show Supplier Material materials with Kobalt of 0.35 - 0.6 % |
Kupfer | Balance |
Technological properties
Property | ||
---|---|---|
Application areas | Typical applications include high reliability automotive terminals and spring contacts for switches and relays. |