Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.36 g/cm³ Show Supplier Material materials with Dichte of 8.36 g/cm³ |
Abmessung
Property | Value |
---|---|
Breite | 1.27 - 406.5 mm Show Supplier Material materials with Breite of 1.27 - 406.5 mm |
Dicke | 0.03 - 0.05 mm Show Supplier Material materials with Dicke of 0.03 - 0.05 mm |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 3 % Show Supplier Material materials with Dehnung of 3 % | min. |
Elastizitätsmodul | 23.0 °C | 131 GPa Show Supplier Material materials with Elastizitätsmodul of 131 GPa | |
Härte, Vickers | 23.0 °C | 325 [-] Show Supplier Material materials with Härte, Vickers of 325 [-] | min. |
Streckgrenze Rp 0,2 | 23.0 °C | 1103 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 1103 MPa | min. |
Zugfestigkeit | 23.0 °C | 1200 MPa Show Supplier Material materials with Zugfestigkeit of 1200 MPa | min. |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.75E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.75E-5 1/K |
Wärmeleitfähigkeit | 23.0 °C | 105 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 105 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Specific Electrical conductivity | 17 - 28 % IACS Show Supplier Material materials with Specific Electrical conductivity of 17 - 28 % IACS | |
spezifischer Widerstand | 23.0 °C | 6.2E-6 - 1.01E-5 Ω·m Show Supplier Material materials with spezifischer Widerstand of 6.2E-6 - 1.01E-5 Ω·m |
Magnetisch
Property | Temperature | Value | Comment |
---|---|---|---|
Relative magnetische Permeabilität | 23.0 °C | 1 [-] Show Supplier Material materials with Relative magnetische Permeabilität of 1 [-] | max. |
Technological properties
Property | ||
---|---|---|
Application areas | EtchMet alloy is a material that is tailor made for the springs in voice coil motors and optical image stabilization systems common in smart phone cameras. |