Allgemein
Property | Value |
---|---|
Dichte | 0.03 - 0.09 g/cm³ Show Material materials with Dichte of 0.03 - 0.09 g/cm³ |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 4.0 - 5.0 % Show Material materials with Dehnung of 4.0 - 5.0 % | |
Zugfestigkeit | 0.2 - 0.9 MPa Show Material materials with Zugfestigkeit of 0.2 - 0.9 MPa | at 4-5% strain |
Thermisch
Property | Value |
---|---|
Wärmeleitfähigkeit | 0.02 - 0.03 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 0.02 - 0.03 W/(m·K) |
Optisch
Property | Value |
---|---|
Transparenz | no |
Technological properties
Property | ||
---|---|---|
Application areas | Insulation applications, automotive interiors | |
Processing methods | Foaming |