Metco 4010B Titanium Grade 4 HDH Wrought Powder

Alternative und Handelsbezeichungen
similar to Metco 4010A, Metco 4010C, Metco 4010D, Metco 4010E (Metco™ 4010 series)
Want to keep this datasheet? Save it now in your required format

Description

Oerlikon Metco’s titanium and titanium alloy powders produce coatings having a range of characteristics not found in any other thermal spray powder materials. The coatings are light in weight with high strength-to-weight ratio and resistant to most corrosives. Titanium readily combines with other metals to form useful alloys. Owing to these suitable mechanochemical properties, pure titanium and titanium alloy powders can be employed in a number of applications via chemical, powder metallurgy and thermal spray processes.


Thermal spray coatings of titanium-based materials are commonly used in medical applications where biologic compatibility is required. Additionally, these coatings may also be used as a potential bond coat for hydroxylapatite coatings that are often used as a top-coat on biomedical implants. Titanium powders may also be used to produce dense, corrosion resistant coatings. Titanium powders have strong affinity and reactivity with oxygen, hydrogen and nitrogen at high temperatures. Most of the thermal spray coatings from these powders are produced under controlled atmosphere conditions (low pressure or soft vacuum).

Related Standards

Diese Materialdaten wurden von Oerlikon Metco zur Verfügung gestellt

Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

Ashby charts

Eigenschaften

Allgemein

PropertyTemperatureValueComment

Partikelgrößenbereich

75 - 180 µm

Show Supplier Material materials with Partikelgrößenbereich of 75 - 180 µm

Schüttdichte

23.0 °C

1.8 - 2.5 g/cm³

Show Supplier Material materials with Schüttdichte of 1.8 - 2.5 g/cm³

apparent density

Thermisch

PropertyValue

Max. Betriebstemperatur

400 °C

Show Supplier Material materials with Max. Betriebstemperatur of 400 °C

Schmelzpunkt

1649 °C

Show Supplier Material materials with Schmelzpunkt of 1649 °C

Chemical properties

PropertyValueComment

Eisen

0.5 %

Show Supplier Material materials with Eisen of 0.5 %

max

Kohlenstoff

0.08 %

Show Supplier Material materials with Kohlenstoff of 0.08 %

max

Sauerstoff

0.4 %

Show Supplier Material materials with Sauerstoff of 0.4 %

max

Stickstoff

0.05 %

Show Supplier Material materials with Stickstoff of 0.05 %

max

Titan

balance

Wasserstoff

0.02 %

Show Supplier Material materials with Wasserstoff of 0.02 %

max

Technological properties

Property
Availability

Stock

Chemical composition

Ti 99.5+

Distribution

Global

Handling recommendations

Store in the original container in a dry location; Open containers should be stored in a drying oven below 38°C (100 °F) to prevent moisture pickup; Tumble contents prior to use to prevent material segregation.

Morphology

Angular / blocky

Order number

1101154

Other

Use coarser pure titanium powders such as Metco 4010B to produce coatings with very high surface roughness and porosity. These types of coatings are often desirable for biomedical implant applications because the porous structure is believed to promote bone growth onto the implants. Grade 4 titanium powders are recommended for use in biomedical applications. For some biomedical applications, layers of both the fine and the coarse powders may be applied serving different functions. HDH powder products are less expensive than atomized powder products.

Packaging size

1.5 kg (approx. 3.3 lb)

Processing history

HDH (hydride-dehydride) process from wrought raw materials

Processing methods

ChamPro™

Safety data sheet

www.oerlikon.com/metco SDS No. 50-2418