Amdry 625 Superalloy Powder for Braze Repair

Alternative und Handelsbezeichungen
similar to Inconel 625 (Inconel is a registered trademark of Huntington Alloys Corp.)
Want to keep this datasheet? Save it now in your required format

Description

Amdry™ nickel and cobalt superalloy powders were developed as complimentary additives for Metco ADB (Activated Diffusion Braze) filler metals, such as Amdry DF-3, DF-4B, DF-6A or BRB, for crack repair and surface restoration. These superalloy products are produced by a dry gas atomization process to assure consistency, purity and conformity to rigid industrial, aerospace and military specifications.


Regardless of the base material that required brazing or repair, the wide range of Metco superalloy powders ensures the right choice and availability.


Metco superalloy products are produced and available as powders. While blending is typically performed by the customer, any ratios desired can be pre-blended for you by Oerlikon Metco. The powders can be delivered pre-blended with braze alloy powders for use with cements or gels. The blends can also be converted to paste, braze tape or braze preforms for a more precise and cost-effective method of application.


Amdry superalloy products do not contain temperature suppressants. Therefore, they are designed not to melt during the braze process, but to form a matrix within the braze joint that is metallurgically compatible with the substrate material.

Diese Materialdaten wurden von Oerlikon Metco zur Verfügung gestellt

Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

Ashby charts

Eigenschaften

Allgemein

PropertyValue

Partikelgrößenbereich

45 - 90 µm

Show Supplier Material materials with Partikelgrößenbereich of 45 - 90 µm

Chemical properties

PropertyValueComment

Andere

3.53 %

Show Supplier Material materials with Andere of 3.53 %

max

Chrom

20 - 23 %

Show Supplier Material materials with Chrom of 20 - 23 %

Eisen

5 %

Show Supplier Material materials with Eisen of 5 %

max

Molybdän

8 - 10 %

Show Supplier Material materials with Molybdän of 8 - 10 %

Nickel

balance

Niob + Tantal

3.15 - 4.15 %

Show Supplier Material materials with Niob + Tantal of 3.15 - 4.15 %

Technological properties

Property
Application areas

Blended in various ratios with ADB braze filler metals for crack repair and surface restoration on superalloy turbine airfoils and other turbine components. General repair and restoration of superalloy-based components. Blended in various ratios with standard braze filler to form excellent wide-gap filler metals.

Availability

Stock

Chemical composition

Ni 21.5Cr 9Mo 3.6(Nb+Ta) 2.5Fe

Distribution

Global

Handling recommendations

Store in the original, closed container in a dry location and Tumble contents prior to use to prevent segregation.

Morphology

Spheroidal

Order number

1001045

Packaging size

5 lb (approx. 2.25 kg)

Processing history

Gas Atomized

Processing methods

Brazing

Safety data sheet

www.oerlikon.com/metco SDS No. 50-310