Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of friction | 0.2 [-] Show Supplier Material materials with Coefficient of friction of 0.2 [-] | ||
Coefficient of friction, kinetic | 0.2 [-] Show Supplier Material materials with Coefficient of friction, kinetic of 0.2 [-] | against steel (0.25m/s, 0.25N/mm) | |
Dichte | 23.0 °C | 0.96 g/cm³ Show Supplier Material materials with Dichte of 0.96 g/cm³ | max., DIN 53479, ISO 1183 |
Moisture absorption | 23.0 °C | 0 % Show Supplier Material materials with Moisture absorption of 0 % | no moisture absorption |
Molmasse | 500000 g/mol Show Supplier Material materials with Molmasse of 500000 g/mol | ||
Wasserabsorption | 23.0 °C | 0.01 % Show Supplier Material materials with Wasserabsorption of 0.01 % | |
Wasseraufnahme, Sättigung | 23.0 °C | 0.01 % Show Supplier Material materials with Wasseraufnahme, Sättigung of 0.01 % | max., DIN 53715, till 96h |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 500 % Show Supplier Material materials with Dehnung of 500 % | min., DIN 53455, ISO 527-2 |
Elastizitätsmodul | 23.0 °C | 0.8 GPa Show Supplier Material materials with Elastizitätsmodul of 0.8 GPa | min., DIN 53457, ISO 527-2 |
Hardness, Ball Indentation | 23.0 °C | 35 MPa Show Supplier Material materials with Hardness, Ball Indentation of 35 MPa | min., DIN 53456, ISO 2039 |
Härte, Shore D | 23.0 °C | 62 - 65 [-] Show Supplier Material materials with Härte, Shore D of 62 - 65 [-] | DIN 868, ISO 7619-1 |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 25 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 25 kJ/m² | min., DIN 53453, ISO 179 |
Streckgrenze | 23.0 °C | 25 MPa Show Supplier Material materials with Streckgrenze of 25 MPa | DIN 53455, ISO 527-2 |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 1.80 MPa | 42 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 42 °C | ISO 75-A | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2E-4 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2E-4 1/K | |||
Max. Betriebstemperatur | 80 - 90 °C Show Supplier Material materials with Max. Betriebstemperatur of 80 - 90 °C | ||||
Max. Betriebstemperatur, fortlaufend | 80 °C Show Supplier Material materials with Max. Betriebstemperatur, fortlaufend of 80 °C | DIN 53446, in air for 20000h | |||
Max. Betriebstemperatur, kurz | 90 °C Show Supplier Material materials with Max. Betriebstemperatur, kurz of 90 °C | in air | |||
Min. Betriebstemperatur | -100 °C Show Supplier Material materials with Min. Betriebstemperatur of -100 °C | ||||
Schmelzpunkt | 130 - 135 °C Show Supplier Material materials with Schmelzpunkt of 130 - 135 °C | ISO 3146 method C | |||
Wärmeformbeständigkeitstemperatur | 42 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 42 °C | ||||
Wärmeleitfähigkeit | 23.0 °C | 0.4 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 0.4 W/(m·K) | DIN 52612 | ||
Entflammbarkeit | UL94: HB, for 3/6mm |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Durchschlagfestigkeit | 23.0 °C | 45 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 45 kV/mm | max., DIN 53481, ISO 60243 |
Surface resistivity | 23.0 °C | 1.00E+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1.00E+12 Ω/sq | min., DIN 53482, ISO 60093 |
Volume resistivity | 23.0 °C | 1.00E+12 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+12 Ω·cm | min., DIN 53482, ISO 60093 |
Technological properties
Property | ||
---|---|---|
Application areas | Food sector, food and drink filling equipment, cutting boards, bumper guards Conveyor: Conveyor elements, Conveyor troughs, Conveyor slide lining, Conveyors stars, Antistatic sliding elements, Curved tracks, Curve guides, Conveyor belts Sliding: Sliding rails, Sliding profiles, Sliding segments Other applications: Wiping strips, Feed hooper, Outlets, Belt stripping, Bins, Gaskets, Format sets, Guiding elements, Sliding elements, Plain bearing, Link belts, Highly wear-resistant sliding elements, Chain guides, Sprockets, Crane support plates, Bearing bushes, Baffle plates, Moulding stripes, Pump parts, Belt guides, Rolls, Chain-pulled conveyors, Control discs, Transport chutes, Deflections pulleys, Wear bars, Workpiece carriers, Toothed wheels, Centrifuges | |
Certifications | Food Contact EU:Yes, FDA:Yes | |
Color | AB Sky Blue | |
Wear resistance | Sand Slurry Test: 350% ISO 15527 |