Allgemein
Property | Temperature | Value |
---|---|---|
Lineare Dichte | 23.0 °C | 3.45E-3 - 4.2E-3 g/cm Show Supplier Material materials with Lineare Dichte of 3.45E-3 - 4.2E-3 g/cm |
Abmessung
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Nominal breaking force | 23.0 °C | 258 N Show Supplier Material materials with Nominal breaking force of 258 N | Tensile Member: E Glass |
Technological properties
Property | ||
---|---|---|
Color | White | |
Cord Construction | 330.1/0 | |
Other | Manufacturing Location: Canada | |
Processing history | Latex Type: NBR, Dip Pick-Up: 11 to 19% | |
Twist per Meter | 52 - 68 TPM | Direction: Z |