Allgemein
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dichte | 1.86 g/cm³ Show Supplier Material materials with Dichte of 1.86 g/cm³ | ASTM D792 | |
Moisture absorption | 0.14 % Show Supplier Material materials with Moisture absorption of 0.14 % | ASTM D570 | Condition D₁-24/23 |
Mechanisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Druckfestigkeit | 206.8 MPa Show Supplier Material materials with Druckfestigkeit of 206.8 MPa | ASTM D638 | Condition E-1/150: T-150 |
241.3 MPa Show Supplier Material materials with Druckfestigkeit of 241.3 MPa | ASTM D638 | Condition A | |
Härte, Rockwell M | 105 [-] Show Supplier Material materials with Härte, Rockwell M of 105 [-] | ASTM D785 | |
Kompressionsmodul | 4.8 GPa Show Supplier Material materials with Kompressionsmodul of 4.8 GPa | ASTM D695 | Condition A |
Zugfestigkeit | 220.6 MPa Show Supplier Material materials with Zugfestigkeit of 220.6 MPa | ASTM D638 | Condition E-1/150: T-150 |
268.9 MPa Show Supplier Material materials with Zugfestigkeit of 268.9 MPa | ASTM D638 | Condition A |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Glasübergangstemperatur | 170 °C Show Supplier Material materials with Glasübergangstemperatur of 170 °C | min. | DMA | |
Relative temperature index, electrical | 200 °C Show Supplier Material materials with Relative temperature index, electrical of 200 °C | ¹ | |
Relative temperature index, mechanical strength | 200 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 200 °C | ¹ | |
Entflammbarkeit | UL Bulletin 94, Class HB |
Elektrisch
Property | Value | Frequency | Testing Standard | Comment |
---|---|---|---|---|
Dielektrizitätskonstante | 4.39 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4.39 [-] | 1MHz | ASTM D150 | Condition A |
4.62 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4.62 [-] | 1MHz | ASTM D150 | Condition D-24/23 | |
4.62 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4.62 [-] | 1MHz | ASTM D150 | Condition D-48/50 | |
Durchschlagfestigkeit | 14.96 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 14.96 kV/mm | ASTM D149 | Condition D-48/50 | |
15.74 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 15.74 kV/mm | ASTM D149 | Condition A | ||
Durchschlagspannung | 55 kV Show Supplier Material materials with Durchschlagspannung of 55 kV | ASTM D149 | Condition A | |
70 kV Show Supplier Material materials with Durchschlagspannung of 70 kV | ASTM D149 | Condition D-48/50 | ||
Verlustfaktor | 0.024 [-] Show Supplier Material materials with Verlustfaktor of 0.024 [-] | 1MHz | ASTM D150 | Condition A |
0.034 [-] Show Supplier Material materials with Verlustfaktor of 0.034 [-] | 1MHz | ASTM D150 | Condition D-24/23 | |
0.04 [-] Show Supplier Material materials with Verlustfaktor of 0.04 [-] | 1MHz | ASTM D150 | Condition D-48/50 |
Technological properties
Property | ||
---|---|---|
Application areas | Typical applications include bushings, spacers and structural parts for power generation equipment. | |
Fillers | Glass Fabric | |
Other | 1.This temperature is a recommendation only, and based upon experience in various applications. The maximum operating temperature is dependent upon the application and should be investigated prior to use 2.The mechanical properties are converted from American unit system to International unit system. | |
Supplier Disclaimer | This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values". To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest. It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available. |