Allgemein
Property | Value | Testing Standard | Comment |
---|---|---|---|
Bonding strength | 1043.3 Kg Show Supplier Material materials with Bonding strength of 1043.3 Kg | ASTM D229 | Condition A |
Dichte | 1.8 g/cm³ Show Supplier Material materials with Dichte of 1.8 g/cm³ | ASTM D792 | |
Moisture absorption | 0.1 % Show Supplier Material materials with Moisture absorption of 0.1 % | ASTM D570 | Condition D₁-24/23 |
Mechanisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Biegefestigkeit | 448.2 MPa Show Supplier Material materials with Biegefestigkeit of 448.2 MPa | ASTM D790 | Condition A, Transverse |
482.6 MPa Show Supplier Material materials with Biegefestigkeit of 482.6 MPa | ASTM D790 | Condition A | |
Biegemodul | 17.2 GPa Show Supplier Material materials with Biegemodul of 17.2 GPa | ASTM D790 | Condition A, Transverse |
19.3 GPa Show Supplier Material materials with Biegemodul of 19.3 GPa | ASTM D790 | Condition A | |
Druckfestigkeit | 613.6 MPa Show Supplier Material materials with Druckfestigkeit of 613.6 MPa | ASTM D695 | Condition A | Flatwise |
Elastizitätsmodul | 35.9 GPa Show Supplier Material materials with Elastizitätsmodul of 35.9 GPa | Condition A, Transverse | |
36.5 GPa Show Supplier Material materials with Elastizitätsmodul of 36.5 GPa | Condition A | ||
Härte, Rockwell M | 114 [-] Show Supplier Material materials with Härte, Rockwell M of 114 [-] | ASTM D785 | |
Impact strength, Izod unnotched, ASTM | 534 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 534 J/m | ASTM D256 | Condition E-48/50, Transverse |
694 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 694 J/m | ASTM D256 | Condition E-48/50 | |
Scherfestigkeit | 165.5 MPa Show Supplier Material materials with Scherfestigkeit of 165.5 MPa | ASTM D732 | Condition A, Transverse |
Zugfestigkeit | 379.2 MPa Show Supplier Material materials with Zugfestigkeit of 379.2 MPa | ASTM D638 | Condition A |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Relative temperature index, electrical | 170 °C Show Supplier Material materials with Relative temperature index, electrical of 170 °C | UL Bulletin 746b¹ | |
Relative temperature index, mechanical strength | 180 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 180 °C | UL Bulletin 746b¹ | |
Arc resistance | 170 seconds, ASTM D495, Condition A | ||
Entflammbarkeit | UL Bulletin 94, Class HB |
Elektrisch
Property | Value | Frequency | Testing Standard | Comment |
---|---|---|---|---|
Dielektrizitätskonstante | 5.1 [-] Show Supplier Material materials with Dielektrizitätskonstante of 5.1 [-] | 1MHz | ASTM D150 | Condition A & D-24/23 |
Durchschlagfestigkeit | 13.77 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 13.77 kV/mm | ASTM D149 | Condition D-48/50 | |
15.75 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 15.75 kV/mm | ASTM D149 | Condition A | ||
Durchschlagspannung | 65 kV Show Supplier Material materials with Durchschlagspannung of 65 kV | ASTM D149 | Condition D-48/50 | |
70 kV Show Supplier Material materials with Durchschlagspannung of 70 kV | ASTM D149 | Condition A | ||
Verlustfaktor | 0.02 [-] Show Supplier Material materials with Verlustfaktor of 0.02 [-] | 1MHz | ASTM D150 | Condition A & D-24/23 |
Technological properties
Property | ||
---|---|---|
Fillers | Glass Fabric | |
Other | 1.This temperature is a recommendation only, and based upon experience in various applications. The maximum operating temperature is dependent upon the application and should be investigated prior to use. | |
Supplier Disclaimer | This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values". To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest. It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available. |