Allgemein
Property | Value | Comment |
---|---|---|
Bonding strength | 997.9 Kg Show Supplier Material materials with Bonding strength of 997.9 Kg | Condition A |
Dichte | 1.8 g/cm³ Show Supplier Material materials with Dichte of 1.8 g/cm³ | |
Moisture absorption | 0.1 % Show Supplier Material materials with Moisture absorption of 0.1 % | Condition D₁-24/23 |
Mechanisch
Property | Value | Comment |
---|---|---|
Biegefestigkeit | 517.1 MPa Show Supplier Material materials with Biegefestigkeit of 517.1 MPa | Condition A |
65000 MPa Show Supplier Material materials with Biegefestigkeit of 65000 MPa | Condition A, Transverse | |
Biegemodul | 16.5 GPa Show Supplier Material materials with Biegemodul of 16.5 GPa | Condition A, Transverse |
18.6 GPa Show Supplier Material materials with Biegemodul of 18.6 GPa | Condition A | |
Druckfestigkeit | 448.2 MPa Show Supplier Material materials with Druckfestigkeit of 448.2 MPa | Condition A | Flatwise |
Härte, Rockwell M | 100 [-] Show Supplier Material materials with Härte, Rockwell M of 100 [-] | |
Impact strength, Izod notched, ASTM | 640.5 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 640.5 J/m | Condition E-48/50, Transverse |
747.3 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 747.3 J/m | Condition E-48/50 | |
Scherfestigkeit | 151.7 MPa Show Supplier Material materials with Scherfestigkeit of 151.7 MPa | Transverse |
Zugfestigkeit | 310.3 MPa Show Supplier Material materials with Zugfestigkeit of 310.3 MPa | Condition A |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Glasübergangstemperatur | 115 °C Show Supplier Material materials with Glasübergangstemperatur of 115 °C | ||
Koeffizient der thermischen Ausdehnung | 1e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1e-05 1/K | ||
1.3e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.3e-05 1/K | Transverse | ||
Relative temperature index, electrical | 130 °C Show Supplier Material materials with Relative temperature index, electrical of 130 °C | ¹ | |
Relative temperature index, mechanical strength | 140 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 140 °C | ¹ | |
Arc resistance | 100 seconds, Condition A | ||
Entflammbarkeit | UL 94, Class HB |
Elektrisch
Property | Value | Frequency | Testing Standard | Comment |
---|---|---|---|---|
Dielektrizitätskonstante | 4.8 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4.8 [-] | 1MHz | Condition D₁-24/23 | |
Durchschlagfestigkeit | 25.98 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 25.98 kV/mm | Condition D-48/50 | ||
26.37 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 26.37 kV/mm | Condition A | |||
Durchschlagspannung | 50 kV Show Supplier Material materials with Durchschlagspannung of 50 kV | ASTM D149 | Condition D-48/50 | |
60 kV Show Supplier Material materials with Durchschlagspannung of 60 kV | ASTM D149 | Condition A | ||
Kriechstromfestigkeit | 150 V Show Supplier Material materials with Kriechstromfestigkeit of 150 V | |||
Verlustfaktor | 0.025 [-] Show Supplier Material materials with Verlustfaktor of 0.025 [-] | 1MHz | Condition D₁-24/23 |
Technological properties
Property | ||
---|---|---|
Application areas | It is used in cryogenic applications. | |
Fillers | Glass Fabric | |
Other | 1.This temperature is a recommendation only, and based upon experience in various applications. The maximum operating temperature is dependent upon the application and should be investigated prior to use 2.The mechanical properties are converted from American unit system to International unit system. | |
Supplier Disclaimer | This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values". To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest. It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available. |