Allgemein
Property | Value | Comment |
---|---|---|
Bonding strength | 181.44 Kg Show Supplier Material materials with Bonding strength of 181.44 Kg | Condition A |
Dichte | 2.18 g/cm³ Show Supplier Material materials with Dichte of 2.18 g/cm³ | |
Moisture absorption | 1.4 % Show Supplier Material materials with Moisture absorption of 1.4 % | Condition D₁-24/23 |
Mechanisch
Property | Value | Comment |
---|---|---|
Biegefestigkeit | 118.6 MPa Show Supplier Material materials with Biegefestigkeit of 118.6 MPa | Condition A, Transverse |
160.0 MPa Show Supplier Material materials with Biegefestigkeit of 160.0 MPa | Condition A | |
Druckfestigkeit | 269 MPa Show Supplier Material materials with Druckfestigkeit of 269 MPa | Condition A | Edgewise |
448.1 MPa Show Supplier Material materials with Druckfestigkeit of 448.1 MPa | Condition A | Flatwise | |
Härte, Rockwell M | 110 [-] Show Supplier Material materials with Härte, Rockwell M of 110 [-] | |
Impact strength, Izod notched, ASTM | 800.7 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 800.7 J/m | Condition E-48/50 |
800.7 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 800.7 J/m | Condition E-48/50, Transverse | |
Zugfestigkeit | 434.4 MPa Show Supplier Material materials with Zugfestigkeit of 434.4 MPa | Condition A |
Thermisch
Property | Value |
---|---|
Entflammbarkeit | UL 94, Class V-0 |
Technological properties
Property | ||
---|---|---|
Application areas | NP504WR is designed for structural applications. | |
Fillers | Glass Fabric | |
Other | The mechanical properties are converted from American unit system to International unit system. | |
Supplier Disclaimer | This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values". To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest. It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available. |