Allgemein
Property | Value | Testing Standard | Comment |
---|---|---|---|
Moisture absorption | 0.07 % Show Supplier Material materials with Moisture absorption of 0.07 % | ASTM D570 | Condition D₁-24/23 |
Mechanisch
Property | Temperature | Value | Testing Standard | Comment |
---|---|---|---|---|
Biegefestigkeit | 448.2 MPa Show Supplier Material materials with Biegefestigkeit of 448.2 MPa | ASTM D790 | Condition A, Transverse | |
130 °C | 420.6 MPa Show Supplier Material materials with Biegefestigkeit of 420.6 MPa | ASTM D790 | ||
140 °C | 417.1 MPa Show Supplier Material materials with Biegefestigkeit of 417.1 MPa | ASTM D790 | ||
155 °C | 365.2 MPa Show Supplier Material materials with Biegefestigkeit of 365.2 MPa | ASTM D790 | ||
Druckfestigkeit | 130 °C | 482.6 MPa Show Supplier Material materials with Druckfestigkeit of 482.6 MPa | ||
140 °C | 462 MPa Show Supplier Material materials with Druckfestigkeit of 462 MPa | |||
155 °C | 496.4 MPa Show Supplier Material materials with Druckfestigkeit of 496.4 MPa | ASTM D695 | ||
Impact strength, Izod unnotched, ASTM | 1227.7 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 1227.7 J/m | ASTM D256 | Condition E-48/50, Transverse | |
1494.6 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 1494.6 J/m | ASTM D256 | Condition E-48/50 |
Elektrisch
Property | Value | Frequency | Testing Standard | Comment |
---|---|---|---|---|
Dielektrizitätskonstante | 4.8 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4.8 [-] | 1MHz | ASTM D150 | |
Durchschlagspannung | 55 kV Show Supplier Material materials with Durchschlagspannung of 55 kV | ASTM D149 | Condition D-48/50 | |
75 kV Show Supplier Material materials with Durchschlagspannung of 75 kV | ASTM D149 | Condition A | ||
Surface resistivity | 2.3e+15 Ω/sq Show Supplier Material materials with Surface resistivity of 2.3e+15 Ω/sq | ASTM D257 | ||
Verlustfaktor | 0.025 [-] Show Supplier Material materials with Verlustfaktor of 0.025 [-] | 1MHz | ASTM D150 | |
Volume resistivity | 6.9e+15 Ω·cm Show Supplier Material materials with Volume resistivity of 6.9e+15 Ω·cm | ASTM D257 |
Technological properties
Property | ||
---|---|---|
Application areas | Ideal material for retaining ring insulation. | |
Fillers | Glass Fabric | |
Other | The mechanical properties are converted from American unit system to International unit system. | |
Supplier Disclaimer | This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values". To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest. It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available. |