Allgemein
Mechanisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Biegefestigkeit | 568.8 MPa Show Supplier Material materials with Biegefestigkeit of 568.8 MPa | ASTM D349 | Condition A |
Druckfestigkeit | 499.9 MPa Show Supplier Material materials with Druckfestigkeit of 499.9 MPa | ASTM D349 | Condition A |
Härte, Rockwell M | 110 [-] Show Supplier Material materials with Härte, Rockwell M of 110 [-] | ASTM D349 | |
Kompressionsmodul | 8.6 GPa Show Supplier Material materials with Kompressionsmodul of 8.6 GPa | ASTM D349 | Condition A |
Zugfestigkeit | 344.7 MPa Show Supplier Material materials with Zugfestigkeit of 344.7 MPa | ASTM D349 | Condition A |
Thermisch
Property | Value |
---|---|
Entflammbarkeit | UL 94, Class HB |
Technological properties
Property | ||
---|---|---|
Application areas | RM271 is used in applications requiring low moisture absorption. | |
Fillers | Glass Fabric | |
Other | The mechanical properties are converted from American unit system to International unit system. | |
Supplier Disclaimer | This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values". To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest. It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available. |