Allgemein
Property | Value | Testing Standard | Comment |
---|---|---|---|
Bonding strength | 1043.26 Kg Show Supplier Material materials with Bonding strength of 1043.26 Kg | ASTM D229 | Condition D-48/50 |
1133.98 Kg Show Supplier Material materials with Bonding strength of 1133.98 Kg | ASTM D229 | Condition A | |
Dichte | 1.37 g/cm³ Show Supplier Material materials with Dichte of 1.37 g/cm³ | ||
Moisture absorption | 3.5 % Show Supplier Material materials with Moisture absorption of 3.5 % | Condition D₁-24/23 |
Mechanisch
Property | Value | Comment |
---|---|---|
Biegefestigkeit | 117.2 MPa Show Supplier Material materials with Biegefestigkeit of 117.2 MPa | Condition A, Transverse |
126.9 MPa Show Supplier Material materials with Biegefestigkeit of 126.9 MPa | Condition A | |
Biegemodul | 10.3 GPa Show Supplier Material materials with Biegemodul of 10.3 GPa | Condition A, Transverse |
11.0 GPa Show Supplier Material materials with Biegemodul of 11.0 GPa | Condition A | |
Druckfestigkeit | 234.4 MPa Show Supplier Material materials with Druckfestigkeit of 234.4 MPa | Condition A |
Härte, Rockwell M | 100 [-] Show Supplier Material materials with Härte, Rockwell M of 100 [-] | |
Impact strength, Izod unnotched, ASTM | 175 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 175 J/m | Condition E-48/50, Transverse |
195 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 195 J/m | Condition E-48/50 | |
Scherfestigkeit | 96.5 MPa Show Supplier Material materials with Scherfestigkeit of 96.5 MPa | Transverse |
Zugfestigkeit | 82.7 MPa Show Supplier Material materials with Zugfestigkeit of 82.7 MPa | Condition A |
Thermisch
Property | Value | Testing Standard | Comment | ||
---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 2e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2e-05 1/K | IPC-TM 650-2.4.24 | |||
2.2e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.2e-05 1/K | IPC-TM 650-2.4.24 | Transverse | |||
Relative temperature index, mechanical strength | 125 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 125 °C | ¹ | |||
Arc resistance | 15 seconds, ASTM D495, Condition A | ||||
Entflammbarkeit | UL 94, Class HB, Condition A |
Elektrisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Durchschlagfestigkeit | 5.91 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 5.91 kV/mm | Condition D48/50 | |
15.75 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 15.75 kV/mm | Condition A | ||
Durchschlagspannung | 5 kV Show Supplier Material materials with Durchschlagspannung of 5 kV | Condition D48/50 | |
20 kV Show Supplier Material materials with Durchschlagspannung of 20 kV | Condition A | ||
Kriechstromfestigkeit | 155 V Show Supplier Material materials with Kriechstromfestigkeit of 155 V | ASTM D3638 |
Technological properties
Property | ||
---|---|---|
Application areas | Applications include spacers for installation of liquid oxygen apparatus where temperatures are as low as minus 320 F. | |
Fillers | Cotton Fabric | |
Other | 1.This temperature is a recommendation only, and based upon experience in various applications. The maximum operating temperature is dependent upon the application and should be investigated prior to use 2.The mechanical properties are converted from American unit system to International unit system. | |
Supplier Disclaimer | This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values". To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest. It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available. |