Allgemein
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dichte | 1.34 g/cm³ Show Supplier Material materials with Dichte of 1.34 g/cm³ | ASTM D349 | |
Moisture absorption | 0.9 % Show Supplier Material materials with Moisture absorption of 0.9 % | ASTM D349 | Condition D₁-24/23 |
Mechanisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Biegefestigkeit | 126.9 MPa Show Supplier Material materials with Biegefestigkeit of 126.9 MPa | ASTM D349 | Condition A |
Druckfestigkeit | 197.2 MPa Show Supplier Material materials with Druckfestigkeit of 197.2 MPa | ASTM D349 | Condition A |
Härte, Rockwell M | 90 [-] Show Supplier Material materials with Härte, Rockwell M of 90 [-] | ASTM D349 | |
Zugfestigkeit | 61.4 MPa Show Supplier Material materials with Zugfestigkeit of 61.4 MPa | ASTM D349 | Condition A |
Technological properties
Property | ||
---|---|---|
Application areas | RM310 is used for mechanical applications, meeting NEMA C requirements. | |
Fillers | Cotton Fabric | |
Other | The mechanical properties are converted from American unit system to International unit system. | |
Supplier Disclaimer | This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values". To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest. It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available. |