Allgemein
Property | Value | Comment |
---|---|---|
Bonding strength | 566.9 Kg Show Supplier Material materials with Bonding strength of 566.9 Kg | Condition D-48/50 |
621.4 Kg Show Supplier Material materials with Bonding strength of 621.4 Kg | Condition A | |
Moisture absorption | 1.19 % Show Supplier Material materials with Moisture absorption of 1.19 % | Condition D₁-24/23 |
Mechanisch
Property | Value | Comment |
---|---|---|
Biegefestigkeit | 148.2 MPa Show Supplier Material materials with Biegefestigkeit of 148.2 MPa | Condition A, Transverse |
151.7 MPa Show Supplier Material materials with Biegefestigkeit of 151.7 MPa | Condition A | |
Impact strength, Izod notched, ASTM | 77.9 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 77.9 J/m | Condition E-48/50, Transverse |
104.6 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 104.6 J/m | Condition E-48/50 |
Thermisch
Property | Value |
---|---|
Entflammbarkeit | UL 94, Class HB |
Elektrisch
Property | Value | Comment |
---|---|---|
Durchschlagspannung | 25 kV Show Supplier Material materials with Durchschlagspannung of 25 kV | Condition A |
Technological properties
Property | ||
---|---|---|
Fillers | Cotton Fabric and PTFE | |
Other | 1.This temperature is a recommendation only, and based upon experience in various applications. The maximum operating temperature is dependent upon the application and should be investigated prior to use 2.The mechanical properties are converted from American unit system to International unit system. | |
Supplier Disclaimer | This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values". To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest. It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available. |