Allgemein
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dichte | 1.42 g/cm³ Show Supplier Material materials with Dichte of 1.42 g/cm³ | ASTM D792 | |
Moisture absorption | 1.7 % Show Supplier Material materials with Moisture absorption of 1.7 % | ASTM D570 | Condition A |
Mechanisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Biegefestigkeit | 131 MPa Show Supplier Material materials with Biegefestigkeit of 131 MPa | ASTM D790 | Condition A, Transverse |
145.5 MPa Show Supplier Material materials with Biegefestigkeit of 145.5 MPa | ASTM D790 | Condition A | |
Biegemodul | 6.6 GPa Show Supplier Material materials with Biegemodul of 6.6 GPa | ASTM D790 | Condition A, Transverse |
6.8 GPa Show Supplier Material materials with Biegemodul of 6.8 GPa | ASTM D790 | Condition A | |
Druckfestigkeit | 270.3 MPa Show Supplier Material materials with Druckfestigkeit of 270.3 MPa | ASTM D695 | Condition A | Flatwise |
Elastizitätsmodul | 9.9 GPa Show Supplier Material materials with Elastizitätsmodul of 9.9 GPa | ASTM D638 | Condition A, Transverse |
10.2 GPa Show Supplier Material materials with Elastizitätsmodul of 10.2 GPa | ASTM D638 | Condition A | |
Härte, Rockwell M | 86 [-] Show Supplier Material materials with Härte, Rockwell M of 86 [-] | ASTM D785 | |
Impact strength, Izod unnotched, ASTM | 181 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 181 J/m | ASTM D256 | Condition E-48/50, Transverse |
224 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 224 J/m | ASTM D256 | Condition E-48/50 | |
Scherfestigkeit | 140.7 MPa Show Supplier Material materials with Scherfestigkeit of 140.7 MPa | ASTM D732 | Condition A, Transverse |
Zugfestigkeit | 95.8 MPa Show Supplier Material materials with Zugfestigkeit of 95.8 MPa | ASTM D638 | Condition A |
Thermisch
Property | Value |
---|---|
Entflammbarkeit | UL 94, Class HB, Condition A |
Technological properties
Property | ||
---|---|---|
Application areas | NP338 is ideal for applications requiring high impact strength and low coefficient of friction such as railway couplers. | |
Fillers | Cotton Fabric and Graphite Powder | |
Supplier Disclaimer | This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values". To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest. It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available. |