Allgemein
Property | Value | Testing Standard | Comment |
---|---|---|---|
Bonding strength | 861.8 Kg Show Supplier Material materials with Bonding strength of 861.8 Kg | ASTM D229 | Condition A |
Dichte | 1.39 g/cm³ Show Supplier Material materials with Dichte of 1.39 g/cm³ | ASTM D792 | |
Moisture absorption | 2.4 % Show Supplier Material materials with Moisture absorption of 2.4 % | ASTM D570 | Condition D₁-24/23 |
Mechanisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Biegefestigkeit | 124.1 MPa Show Supplier Material materials with Biegefestigkeit of 124.1 MPa | ASTM D790 | Condition A, Transverse |
164.1 MPa Show Supplier Material materials with Biegefestigkeit of 164.1 MPa | ASTM D790 | Condition A | |
Biegemodul | 7.6 GPa Show Supplier Material materials with Biegemodul of 7.6 GPa | ASTM D790 | Condition A, Transverse |
10.3 GPa Show Supplier Material materials with Biegemodul of 10.3 GPa | ASTM D790 | Condition A | |
Druckfestigkeit | 268.9 MPa Show Supplier Material materials with Druckfestigkeit of 268.9 MPa | ASTM D695 | Condition A | Flatwise |
Härte, Rockwell M | 103 [-] Show Supplier Material materials with Härte, Rockwell M of 103 [-] | ASTM D785 | |
Impact strength, Izod unnotched, ASTM | 69 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 69 J/m | ASTM D256 | Condition E-48/50, Transverse |
85 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 85 J/m | ASTM D256 | Condition E-48/50 | |
Scherfestigkeit | 100 MPa Show Supplier Material materials with Scherfestigkeit of 100 MPa | ASTM D732 | Condition A, Transverse |
Zugfestigkeit | 96.5 MPa Show Supplier Material materials with Zugfestigkeit of 96.5 MPa | ASTM D638 | Condition A |
Thermisch
Property | Value | Testing Standard | Comment | ||
---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 1e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1e-05 1/K | IPC-TM 650-2.4.24 | |||
1.2e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.2e-05 1/K | IPC-TM 650-2.4.24 | Transverse | |||
Relative temperature index, electrical | 130 °C Show Supplier Material materials with Relative temperature index, electrical of 130 °C | UL Bulletin 746b¹ | |||
Relative temperature index, mechanical strength | 130 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 130 °C | UL Bulletin 746b¹ | |||
Entflammbarkeit | UL Bulletin 94, Class HB, Condition A |
Elektrisch
Technological properties
Property | ||
---|---|---|
Application areas | BP21NPM is used in applications where reduced wear is needed in non-conductive applications. | |
Fillers | Cotton Fabric and MoS2 | |
Other | 1.This temperature is a recommendation only, and based upon experience in various applications. The maximum operating temperature is dependent upon the application and should be investigated prior to use | |
Supplier Disclaimer | This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values". To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest. It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available. |