Allgemein
Property | Value | Comment |
---|---|---|
Bonding strength | 408.2 Kg Show Supplier Material materials with Bonding strength of 408.2 Kg | |
Dichte | 1.4 g/cm³ Show Supplier Material materials with Dichte of 1.4 g/cm³ | |
Moisture absorption | 0.37 - 0.6 % Show Supplier Material materials with Moisture absorption of 0.37 - 0.6 % | Condition D₁-24/23 | Depending on the thickness of the specimen |
Mechanisch
Property | Value | Comment |
---|---|---|
Biegefestigkeit | 191.0 MPa Show Supplier Material materials with Biegefestigkeit of 191.0 MPa | |
193.1 MPa Show Supplier Material materials with Biegefestigkeit of 193.1 MPa | Transverse | |
Druckfestigkeit | 304.1 MPa Show Supplier Material materials with Druckfestigkeit of 304.1 MPa | Flatwise |
Härte, Rockwell M | 115 [-] Show Supplier Material materials with Härte, Rockwell M of 115 [-] | |
Impact strength, Izod unnotched, ASTM | 29.9 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 29.9 J/m | Transverse |
34.7 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 34.7 J/m | ||
Zugfestigkeit | 116.5 MPa Show Supplier Material materials with Zugfestigkeit of 116.5 MPa |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Glasübergangstemperatur | 130 °C Show Supplier Material materials with Glasübergangstemperatur of 130 °C | min. | DSC | |
145 °C Show Supplier Material materials with Glasübergangstemperatur of 145 °C | max. | DMA | ||
Relative temperature index, electrical | 140 °C Show Supplier Material materials with Relative temperature index, electrical of 140 °C | ¹ | |
Relative temperature index, mechanical strength | 140 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 140 °C | ¹ | |
Arc resistance | 120 seconds | ||
Entflammbarkeit | UL 94, Class HB |
Elektrisch
Property | Value | Frequency | Testing Standard | Comment |
---|---|---|---|---|
Dielektrizitätskonstante | 4.5 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4.5 [-] | 1MHz | ASTM D150 | Condition D-24/23 |
6.6 [-] Show Supplier Material materials with Dielektrizitätskonstante of 6.6 [-] | 1MHz | ASTM D150 | Condition A | |
Durchschlagfestigkeit | 6.69 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 6.69 kV/mm | |||
Durchschlagspannung | 6 kV Show Supplier Material materials with Durchschlagspannung of 6 kV | ASTM D149 | Condition D48/50 | |
65 kV Show Supplier Material materials with Durchschlagspannung of 65 kV | ASTM D149 | Condition A | ||
Kriechstromfestigkeit | 150 V Show Supplier Material materials with Kriechstromfestigkeit of 150 V | |||
Verlustfaktor | 0.054 [-] Show Supplier Material materials with Verlustfaktor of 0.054 [-] | 1MHz | Condition A | |
0.057 [-] Show Supplier Material materials with Verlustfaktor of 0.057 [-] | 1MHz | Condition D-24/23 |
Technological properties
Property | ||
---|---|---|
Application areas | It is designed to be used in tap changers, coil support plates and terminal panels for transformers and their accessories. | |
Fillers | Paper | |
Other | 1.This temperature is a recommendation only, and based upon experience in various applications. The maximum operating temperature is dependent upon the application and should be investigated prior to use 2.The mechanical properties are converted from American unit system to International unit system. | |
Supplier Disclaimer | This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values". To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest. It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available. |