Allgemein
Property | Value | Testing Standard | Comment |
---|---|---|---|
Bonding strength | 635 Kg Show Supplier Material materials with Bonding strength of 635 Kg | ASTM D229 | Condition A |
Dichte | 1.41 g/cm³ Show Supplier Material materials with Dichte of 1.41 g/cm³ | ASTM D792 | |
Moisture absorption | 3 % Show Supplier Material materials with Moisture absorption of 3 % | ASTM D570 | Condition D₁-24/23 |
Mechanisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Biegefestigkeit | 96.5 MPa Show Supplier Material materials with Biegefestigkeit of 96.5 MPa | ASTM D790 | Condition A, Transverse |
137.9 MPa Show Supplier Material materials with Biegefestigkeit of 137.9 MPa | ASTM D790 | Condition A | |
Biegemodul | 6.9 GPa Show Supplier Material materials with Biegemodul of 6.9 GPa | ASTM D790 | Condition A, Transverse |
8.3 GPa Show Supplier Material materials with Biegemodul of 8.3 GPa | ASTM D790 | Condition A | |
Druckfestigkeit | 124.1 MPa Show Supplier Material materials with Druckfestigkeit of 124.1 MPa | ASTM D695 | Condition A | Flatwise |
Härte, Rockwell M | 89 [-] Show Supplier Material materials with Härte, Rockwell M of 89 [-] | ASTM D785 | |
Impact strength, Izod unnotched, ASTM | 30 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 30 J/m | ASTM D256 | Condition E-48/50, Transverse |
31 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 31 J/m | ASTM D256 | Condition E-48/50 | |
Scherfestigkeit | 81.4 MPa Show Supplier Material materials with Scherfestigkeit of 81.4 MPa | ASTM D732 | Condition A, Transverse |
Zugfestigkeit | 86.2 MPa Show Supplier Material materials with Zugfestigkeit of 86.2 MPa | ASTM D638 | Condition A |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Relative temperature index, electrical | 120 °C Show Supplier Material materials with Relative temperature index, electrical of 120 °C | UL Bulletin 746b¹ | |
Relative temperature index, mechanical strength | 120 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 120 °C | UL Bulletin 746b¹ | |
Arc resistance | 110 seconds, ASTM D495, Condition A | ||
Entflammbarkeit | UL Bulletin 94, Class HB, Condition A |
Elektrisch
Property | Value | Frequency | Testing Standard | Comment |
---|---|---|---|---|
Dielektrizitätskonstante | 6.49 [-] Show Supplier Material materials with Dielektrizitätskonstante of 6.49 [-] | 1MHz | ASTM D150 | Condition D-24/23 |
Durchschlagfestigkeit | 27.56 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 27.56 kV/mm | ASTM D149 | Condition A | |
Durchschlagspannung | 10 kV Show Supplier Material materials with Durchschlagspannung of 10 kV | ASTM D149 | Condition D48/50 | |
55 kV Show Supplier Material materials with Durchschlagspannung of 55 kV | ASTM D149 | Condition A | ||
Verlustfaktor | 0.096 [-] Show Supplier Material materials with Verlustfaktor of 0.096 [-] | 1MHz | ASTM D150 | Condition D-24/23 |
Technological properties
Property | ||
---|---|---|
Application areas | Intended for applications where electrical and moisture requirements are secondary. | |
Fillers | Paper | |
Other | 1.This temperature is a recommendation only, and based upon experience in various applications. The maximum operating temperature is dependent upon the application and should be investigated prior to use | |
Supplier Disclaimer | This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values". To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest. It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available. |