Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 2.7 g/cm³ Show Supplier Material materials with Dichte of 2.7 g/cm³ |
Abmessung
Property | Value | Comment |
---|---|---|
Breite | 1943 mm Show Supplier Material materials with Breite of 1943 mm | max. |
Dicke | 6.35 - 101.6 mm Show Supplier Material materials with Dicke of 6.35 - 101.6 mm | |
Länge | 8990 mm Show Supplier Material materials with Länge of 8990 mm | max. |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 28 % Show Supplier Material materials with Dehnung of 28 % |
Elastizitätsmodul | 23.0 °C | 68.9 GPa Show Supplier Material materials with Elastizitätsmodul of 68.9 GPa |
Streckgrenze | 23.0 °C | 28 MPa Show Supplier Material materials with Streckgrenze of 28 MPa |
Zugfestigkeit | 23.0 °C | 83 MPa Show Supplier Material materials with Zugfestigkeit of 83 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.38E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.38E-5 1/K | for 23-100°C |
Wärmeleitfähigkeit | 23.0 °C | 234 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 234 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 3.57E+7 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 3.57E+7 S/m |
Specific Electrical conductivity | 61.5 % IACS Show Supplier Material materials with Specific Electrical conductivity of 61.5 % IACS |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | Balance | ||
Bor | 6E-3 % Show Supplier Material materials with Bor of 6E-3 % | max. | |
Chrom | 3E-3 % Show Supplier Material materials with Chrom of 3E-3 % | max. | |
Eisen | 0.1 - 0.18 % Show Supplier Material materials with Eisen of 0.1 - 0.18 % | ||
Gallium | 0.02 % Show Supplier Material materials with Gallium of 0.02 % | max. | |
Kupfer | 0.01 % Show Supplier Material materials with Kupfer of 0.01 % | max. | |
Magnesium | 0.01 % Show Supplier Material materials with Magnesium of 0.01 % | max | |
Mangan | 3E-3 % Show Supplier Material materials with Mangan of 3E-3 % | max. | |
Silizium | 0.07 % Show Supplier Material materials with Silizium of 0.07 % | max. | |
Titan | 4E-3 % Show Supplier Material materials with Titan of 4E-3 % | max., Ti+V | |
Vanadium | 4E-3 % Show Supplier Material materials with Vanadium of 4E-3 % | max. | |
Zink | 0.03 % Show Supplier Material materials with Zink of 0.03 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | This product is especially suitable for electrical applications. It is used for bus bar manufacturing that specializes in the transport and the distribution of electricity. PCP Aluminium developed this product to meet complex electrical requirements in order to minimize energy loss. This product is available in a variety of sizes. | |
Availability | Other thicknesses, widhts and lengths may be available upon inquiry. On request, this product may be milled and coated with protective plastic film on the milled sides. | |
Dimensional stability | Excellent | |
Other | AA1370 is the best aluminium you can get for electrical applications: It is made of prime metal without any recycled alloying material. AA1370 is a subset of AA1350 aluminium. 99.7% pure aluminium ensures increased conductivity. PCP aluminium AA1370-50 is annealed (0) since it becomes less prone to deformation with a stress relief heat treatment. | |
Processing history | Fabricated from prime aluminium cast ingots | |
Welding | Excellent weldability |