Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 2.66 g/cm³ Show Supplier Material materials with Dichte of 2.66 g/cm³ | |
Oberflächenrauigkeit | 25.4 μm Show Supplier Material materials with Oberflächenrauigkeit of 25.4 μm | max. |
Abmessung
Property | Value | Comment |
---|---|---|
Breite | 2591 mm Show Supplier Material materials with Breite of 2591 mm | max. |
Dicke | 6.35 - 101.6 mm Show Supplier Material materials with Dicke of 6.35 - 101.6 mm | |
Länge | 8990 mm Show Supplier Material materials with Länge of 8990 mm | max. |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 16 % Show Supplier Material materials with Dehnung of 16 % |
Elastizitätsmodul | 23.0 °C | 71 GPa Show Supplier Material materials with Elastizitätsmodul of 71 GPa |
Härte, Brinell | 23.0 °C | 70 [-] Show Supplier Material materials with Härte, Brinell of 70 [-] |
Streckgrenze | 23.0 °C | 124 MPa Show Supplier Material materials with Streckgrenze of 124 MPa |
Zugfestigkeit | 23.0 °C | 283 MPa Show Supplier Material materials with Zugfestigkeit of 283 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.38E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.38E-5 1/K | for 23-100°C |
Wärmeleitfähigkeit | 23.0 °C | 120 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 120 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 1.57E+7 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 1.57E+7 S/m |
Specific Electrical conductivity | 27 % IACS Show Supplier Material materials with Specific Electrical conductivity of 27 % IACS |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | Balance | ||
Chrom | 0.05 - 0.25 % Show Supplier Material materials with Chrom of 0.05 - 0.25 % | ||
Eisen | 0.4 % Show Supplier Material materials with Eisen of 0.4 % | max. | |
Kupfer | 0.1 % Show Supplier Material materials with Kupfer of 0.1 % | max. | |
Magnesium | 4 - 4.9 % Show Supplier Material materials with Magnesium of 4 - 4.9 % | ||
Mangan | 0.4 - 1 % Show Supplier Material materials with Mangan of 0.4 - 1 % | ||
Silizium | 0.4 % Show Supplier Material materials with Silizium of 0.4 % | max. | |
Titan | 0.15 % Show Supplier Material materials with Titan of 0.15 % | max., Zr+Ti | |
Zink | 0.25 % Show Supplier Material materials with Zink of 0.25 % | max. | |
Zirkonium | 0.15 % Show Supplier Material materials with Zirkonium of 0.15 % | max., Zr+Ti |
Technological properties
Property | ||
---|---|---|
Anodizing | Hard anodizing: Excellent; Decorative: Not suitable | |
Application areas | Robotic component, Rubber & Plastic mold, Vacuum chamber, Prototyping, Jig, Template | |
Availability | MAX5® mold products are available in temper O3 (homogenized) aluminum in the following size: | |
Corrosion properties | Inland atmosphere: Excellent; Marine atmosphere: Good | |
Dimensional stability | Excellent | |
General machinability | Excellent | |
Polishing ability | Very good | |
Welding | WIG/MIG: very good; By resistance: very good |