Allgemein
Property | Value | Testing Standard |
---|---|---|
Dichte | 1.06 - 1.12 g/cm³ Show Supplier Material materials with Dichte of 1.06 - 1.12 g/cm³ | ASTM D792 |
Mechanisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dehnung | 113 % Show Supplier Material materials with Dehnung of 113 % | ASTM D412 | 500 mm/min |
Härte, Shore A | 67 - 73 [-] Show Supplier Material materials with Härte, Shore A of 67 - 73 [-] | ASTM D2240 | |
Modul bei 100 % Dehnung | 0.00174 GPa Show Supplier Material materials with Modul bei 100 % Dehnung of 0.00174 GPa | ASTM D412 | 500 mm/min |
Reißfestigkeit | 8.5 kN/m Show Supplier Material materials with Reißfestigkeit of 8.5 kN/m | ASTM D624 Die C | 500 mm/min |
Zugfestigkeit | 1.8 MPa Show Supplier Material materials with Zugfestigkeit of 1.8 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzmassenflussrate | 30.1 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 30.1 g/10min | ASTM D1238 | 190°C/2.16kg |
Schrumpfung | 0.9 - 1.5 % Show Supplier Material materials with Schrumpfung of 0.9 - 1.5 % | ASTM D955 | |
0.9 - 1.5 % Show Supplier Material materials with Schrumpfung of 0.9 - 1.5 % | ASTM D955 | Transverse |
Technological properties
Property | ||
---|---|---|
Application areas | Bicycle grip, tool grip, pen grip, toothbrush | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3 | |
Color | White | |
Fillers | Calcium Carbonate | |
Other | Overmolding capabilities: PP |