Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.14 g/cm³ Show Supplier Material materials with Dichte of 1.14 g/cm³ | ASTM D792 |
Wasseraufnahme, Gleichgewicht | 23.0 °C | 0.3 % Show Supplier Material materials with Wasseraufnahme, Gleichgewicht of 0.3 % | max., ASTM D4442 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 110 MPa Show Supplier Material materials with Biegefestigkeit of 110 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 2.7 GPa Show Supplier Material materials with Biegemodul of 2.7 GPa | ASTM D790 |
Dehnung | 23.0 °C | 10 % Show Supplier Material materials with Dehnung of 10 % | min., ASTM D638 |
Härte, Shore D | 23.0 °C | 78 [-] Show Supplier Material materials with Härte, Shore D of 78 [-] | ASTM D2240 |
Impact strength, Izod notched, ASTM | 23.0 °C | 50 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 50 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 67 MPa Show Supplier Material materials with Zugfestigkeit of 67 MPa | ASTM D638 |
Thermisch
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 80 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 80 g/10min | min., ASTM D1238 | |
Schrumpfung | 23.0 °C | 1.2 - 1.6 % Show Supplier Material materials with Schrumpfung of 1.2 - 1.6 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Buckle pull ring, Baby Strollers, Electrical and electronic parts, Information technology equipment parts, Tool housing, Sports equipment, Bicycles-Chain Cover, Gear, Automobiles parts. | |
Color | Black |